Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.310 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.010 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.33 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
MgP4 + Mg3P2 + Sn
Band Gap
1.215 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.000 315.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.003 175.4
InSb (mp-20012) <1 0 0> <0 0 1> 0.007 175.4
GaN (mp-804) <1 0 1> <0 0 1> 0.009 210.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.013 175.4
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.016 280.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.019 315.6
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.026 276.0
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.026 232.2
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.029 138.0
CdS (mp-672) <0 0 1> <0 0 1> 0.030 245.5
Au (mp-81) <1 0 0> <0 0 1> 0.030 35.1
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.035 315.6
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.037 292.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.041 175.4
Ag (mp-124) <1 1 0> <1 1 0> 0.047 97.6
LiF (mp-1138) <1 0 0> <0 0 1> 0.052 280.6
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.054 77.4
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.064 245.5
Al (mp-134) <1 0 0> <0 0 1> 0.067 280.6
InP (mp-20351) <1 0 0> <0 0 1> 0.068 35.1
C (mp-66) <1 0 0> <0 0 1> 0.072 315.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.075 138.0
Au (mp-81) <1 1 0> <1 1 0> 0.076 97.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.081 175.4
Ag (mp-124) <1 0 0> <0 0 1> 0.082 35.1
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.090 245.5
GaSe (mp-1943) <1 1 0> <1 0 1> 0.098 232.2
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.098 315.6
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.109 154.8
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.112 276.0
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.120 280.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.121 175.4
Mg (mp-153) <1 0 1> <0 0 1> 0.121 210.4
Ni (mp-23) <1 0 0> <1 0 1> 0.123 232.2
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.134 175.4
TePb (mp-19717) <1 0 0> <0 0 1> 0.135 175.4
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.139 315.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.148 315.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.158 350.7
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.165 70.1
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.172 207.0
Au (mp-81) <1 1 1> <0 0 1> 0.174 245.5
Al2O3 (mp-1143) <1 0 0> <1 0 1> 0.180 309.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.193 315.6
SiC (mp-11714) <1 0 0> <0 0 1> 0.210 350.7
CsI (mp-614603) <1 0 0> <0 0 1> 0.231 315.6
CdSe (mp-2691) <1 0 0> <0 0 1> 0.234 315.6
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.252 140.3
KCl (mp-23193) <1 1 0> <1 0 1> 0.259 232.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
81 43 47 0 0 0
43 81 47 0 0 0
47 47 77 0 0 0
0 0 0 37 0 0
0 0 0 0 37 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
20.6 -5.9 -8.8 0 0 0
-5.9 20.6 -8.8 0 0 0
-8.8 -8.8 23.5 0 0 0
0 0 0 26.8 0 0
0 0 0 0 26.8 0
0 0 0 0 0 29.2
Shear Modulus GV
29 GPa
Bulk Modulus KV
57 GPa
Shear Modulus GR
25 GPa
Bulk Modulus KR
57 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
57 GPa
Elastic Anisotropy
0.74
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CdSnAs2 (mp-3829) 0.0105 0.000 3
ZnGeAs2 (mp-4008) 0.0154 0.000 3
CdSnSb2 (mp-10063) 0.0114 0.000 3
ZnGeP2 (mp-4524) 0.0142 0.000 3
AlCuSe2 (mp-8016) 0.0102 0.000 3
FeCu2GeS4 (mp-917359) 0.0099 0.037 4
CoCu2GeS4 (mp-6498) 0.0312 0.055 4
CoCu2GeS4 (mp-560428) 0.0371 0.055 4
FeCu2GeS4 (mp-22053) 0.0138 0.037 4
FeCu2GeSe4 (mp-1087471) 0.0692 0.037 4
ZrO (mp-33088) 0.0353 0.424 2
CoO (mp-557513) 0.0353 0.000 2
ZnNi (mp-567903) 0.0353 1.083 2
CuS (mp-760381) 0.0332 0.013 2
CoO (mp-24864) 0.0353 0.000 2
Si (mp-149) 0.0353 0.000 1
Sn (mp-117) 0.0353 0.000 1
C (mp-66) 0.0353 0.136 1
Ge (mp-32) 0.0353 0.000 1
Se (mp-12771) 0.0353 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Sn_d P
Final Energy/Atom
-4.4188 eV
Corrected Energy
-35.3504 eV
Uncorrected energy = -35.3504 eV Corrected energy = -35.3504 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)