Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.147 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.147 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.36 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Sn + Si
Band Gap
0.411 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <1 0 0> 0.001 294.7
C (mp-66) <1 0 0> <1 0 0> 0.003 331.5
Ni (mp-23) <1 1 0> <1 1 0> 0.003 52.1
Ni (mp-23) <1 1 1> <1 1 1> 0.003 63.8
Al (mp-134) <1 0 0> <1 0 0> 0.008 147.3
Al (mp-134) <1 1 0> <1 1 0> 0.008 208.4
Au (mp-81) <1 0 0> <1 0 0> 0.008 294.7
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.030 294.7
SiC (mp-11714) <0 0 1> <1 1 1> 0.032 255.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.033 156.3
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.034 147.3
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.036 208.4
SiC (mp-7631) <0 0 1> <1 1 1> 0.037 255.2
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.046 191.4
ZnO (mp-2133) <0 0 1> <1 1 1> 0.050 255.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.057 294.7
AlN (mp-661) <0 0 1> <1 0 0> 0.065 294.7
NaCl (mp-22862) <1 0 0> <1 0 0> 0.067 294.7
Ni (mp-23) <1 0 0> <1 1 0> 0.075 260.5
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.080 73.7
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.085 104.2
KCl (mp-23193) <1 0 0> <1 0 0> 0.101 331.5
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.112 294.7
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.113 156.3
ZnO (mp-2133) <1 0 1> <1 0 0> 0.118 221.0
Ge (mp-32) <1 0 0> <1 0 0> 0.121 294.7
GaN (mp-804) <1 0 0> <1 0 0> 0.123 184.2
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.123 147.3
Si (mp-149) <1 0 0> <1 0 0> 0.131 147.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.158 36.8
LaF3 (mp-905) <1 0 0> <1 1 1> 0.162 319.0
TiO2 (mp-390) <0 0 1> <1 0 0> 0.168 73.7
MgO (mp-1265) <1 1 0> <1 1 0> 0.169 52.1
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.177 221.0
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.181 208.4
Mg (mp-153) <1 0 0> <1 0 0> 0.183 184.2
C (mp-66) <1 1 0> <1 1 0> 0.187 312.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.203 147.3
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.215 184.2
LiF (mp-1138) <1 1 0> <1 1 0> 0.217 208.4
LiF (mp-1138) <1 1 1> <1 1 1> 0.221 255.2
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.222 255.2
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.233 208.4
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.265 257.9
Mg (mp-153) <1 1 0> <1 1 0> 0.267 312.6
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.275 156.3
PbS (mp-21276) <1 0 0> <1 0 0> 0.279 36.8
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.280 147.3
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.284 257.9
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.295 255.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
97 40 40 0 0 0
40 97 40 0 0 0
40 40 97 0 0 0
0 0 0 46 0 0
0 0 0 0 46 0
0 0 0 0 0 46
Compliance Tensor Sij (10-12Pa-1)
13.6 -4 -4 0 0 0
-4 13.6 -4 0 0 0
-4 -4 13.6 0 0 0
0 0 0 21.6 0 0
0 0 0 0 21.6 0
0 0 0 0 0 21.6
Shear Modulus GV
39 GPa
Bulk Modulus KV
59 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
59 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
59 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn3CrS4 (mp-1080726) 0.0175 0.324 3
Zn3CrSe4 (mp-1095028) 0.0124 0.339 3
Zn3CrTe4 (mp-1087545) 0.0105 0.331 3
CdSnSb2 (mp-10063) 0.0250 0.000 3
GaCuS2 (mp-5238) 0.0192 0.000 3
FeCu2GeS4 (mp-917359) 0.0383 0.185 4
CoCu2GeS4 (mp-6498) 0.0382 0.055 4
CoCu2GeS4 (mp-560428) 0.0476 0.055 4
FeCu2GeS4 (mp-22053) 0.0260 0.185 4
FeCu2GeSe4 (mp-1087471) 0.0871 0.035 4
FeN (mp-6988) 0.0000 0.000 2
ZrC (mp-1009894) 0.0000 0.613 2
NbC (mp-1009458) 0.0000 0.593 2
RuN (mp-1009770) 0.0000 0.071 2
VN (mp-1001839) 0.0000 0.327 2
O2 (mp-1057818) 0.0000 1.882 1
Si (mp-149) 0.0000 0.000 1
Sn (mp-117) 0.0000 0.000 1
C (mp-66) 0.0000 0.136 1
Se (mp-12771) 0.0000 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Sn_d
Final Energy/Atom
-4.5609 eV
Corrected Energy
-9.1219 eV
-9.1219 eV = -9.1219 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 184676
Submitted by
User remarks:
  • Silicon tin (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)