material

SnSb

ID:

mp-10635

DOI:

10.17188/1187247


Tags: Tin antimonide (1/1) Tin antimonide (1/1) - HP Stistaite High pressure experimental phase

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.084 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.75 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 52303 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.000 66.2
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.000 54.1
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.000 38.2
InAs (mp-20305) <1 1 1> <1 1 1> 0.000 66.2
InAs (mp-20305) <1 1 0> <1 1 0> 0.000 54.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.001 38.2
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.001 66.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.003 344.2
C (mp-66) <1 1 1> <1 1 1> 0.003 66.2
C (mp-66) <1 1 0> <1 1 0> 0.003 54.1
CdS (mp-672) <0 0 1> <1 1 1> 0.003 198.7
SiC (mp-8062) <1 1 0> <1 1 0> 0.005 54.1
SiC (mp-8062) <1 0 0> <1 0 0> 0.005 38.2
SiC (mp-7631) <1 1 0> <1 1 0> 0.006 162.3
SiC (mp-7631) <1 0 1> <1 0 0> 0.007 191.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.008 306.0
Al (mp-134) <1 1 1> <1 1 1> 0.012 198.7
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.012 198.7
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.013 191.2
Ni (mp-23) <1 0 0> <1 0 0> 0.018 306.0
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.019 153.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.026 306.0
AlN (mp-661) <0 0 1> <1 1 1> 0.035 265.0
Mg (mp-153) <0 0 1> <1 0 0> 0.036 306.0
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.039 198.7
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.042 198.7
CdSe (mp-2691) <1 1 1> <1 1 1> 0.043 66.2
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.044 162.3
CdSe (mp-2691) <1 1 0> <1 1 0> 0.045 54.1
GaP (mp-2490) <1 0 0> <1 0 0> 0.050 153.0
ZnO (mp-2133) <0 0 1> <1 1 1> 0.051 66.2
C (mp-66) <1 0 0> <1 1 0> 0.051 270.4
CdSe (mp-2691) <1 0 0> <1 0 0> 0.051 38.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.053 306.0
GaN (mp-804) <1 1 0> <1 1 0> 0.058 324.5
GaN (mp-804) <1 1 1> <1 0 0> 0.064 153.0
GaSb (mp-1156) <1 1 1> <1 1 1> 0.064 66.2
GaSb (mp-1156) <1 1 0> <1 1 0> 0.067 54.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.070 306.0
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.070 66.2
WS2 (mp-224) <0 0 1> <1 0 0> 0.070 306.0
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.076 191.2
SiC (mp-8062) <1 1 1> <1 0 0> 0.076 267.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.076 38.2
Mg (mp-153) <1 1 1> <1 0 0> 0.084 153.0
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.084 66.2
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.085 66.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.088 267.7
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.092 344.2
GaN (mp-804) <1 0 1> <1 1 0> 0.093 270.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
111 20 20 0 0 0
20 111 20 0 0 0
20 20 111 0 0 0
0 0 0 14 0 0
0 0 0 0 14 0
0 0 0 0 0 14
Compliance Tensor Sij (10-12Pa-1)
9.5 -1.4 -1.4 0 0 0
-1.4 9.5 -1.4 0 0 0
-1.4 -1.4 9.5 0 0 0
0 0 0 70.6 0 0
0 0 0 0 70.6 0
0 0 0 0 0 70.6
Shear Modulus GV
27 GPa
Bulk Modulus KV
50 GPa
Shear Modulus GR
20 GPa
Bulk Modulus KR
50 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
50 GPa
Elastic Anisotropy
1.85
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrCdO2 (mp-1018032) 0.0210 0.028 3
CaAgO2 (mp-997030) 0.0210 0.031 3
KNaH2 (mp-1007637) 0.0231 0.055 3
BaCaO2 (mp-1018097) 0.0233 0.199 3
RbNaH2 (mp-999274) 0.0231 0.105 3
NiCl (mp-1021674) 0.0191 0.552 2
UP (mp-2011) 0.0048 0.000 2
UN (mp-1865) 0.0150 0.000 2
PdN (mp-1009548) 0.0213 0.952 2
CrN (mp-1000440) 0.0195 0.048 2
Bi (mp-567597) 0.0191 0.050 1
Fe (mp-568345) 0.0233 0.761 1
Ba (mp-639747) 0.0238 0.296 1
U (mp-1056699) 0.0171 0.166 1
S (mp-10869) 0.0048 0.626 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Tin-antimony nanoparticles were prepared by the simple co-precipitation technique. Stoichiometric amounts of metal chlorides of tin and antimony and tri-sodium citrate were dissolved in 40ml distille [...]
The SnSb deposits on Cu foil was obtained by electro-co-deposition in a two-electrode glass cell. An aqueous solution formed by 22.0g/L SnSO4, 16.0g/L KSbOC4H4O61/2H2O, 115.0g/L K4P2O710H2O and 0 [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition SnSb.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sn_d Sb
Final Energy/Atom
-4.0572 eV
Corrected Energy
-8.3064 eV
Uncorrected energy = -8.1144 eV Composition-based energy adjustment (-0.192 eV/atom x 1.0 atoms) = -0.1920 eV Corrected energy = -8.3064 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 52303
  • 52294
Submitted by
User remarks:
  • Tin antimonide (1/1) - HP
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)