material

Sn

ID:

mp-117

DOI:

10.17188/1188292


Tags: Tin - alpha, LT Tin Tin - grey, alpha Tin grey Tin - alpha

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.37 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 40039 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaAs (mp-2534) <1 1 0> <1 1 0> 0.002 187.4
GaAs (mp-2534) <1 1 1> <1 1 1> 0.002 229.5
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.002 306.0
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.003 44.2
Ge (mp-32) <1 1 0> <1 1 0> 0.003 187.4
Ge (mp-32) <1 1 1> <1 1 1> 0.003 229.5
Ni (mp-23) <1 0 0> <1 0 0> 0.004 220.9
AlN (mp-661) <0 0 1> <1 1 1> 0.004 76.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.006 76.5
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.007 306.0
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.007 309.2
InSb (mp-20012) <1 0 0> <1 0 0> 0.008 44.2
InSb (mp-20012) <1 1 0> <1 1 0> 0.008 62.5
InSb (mp-20012) <1 1 1> <1 1 1> 0.008 76.5
InP (mp-20351) <1 0 0> <1 0 0> 0.008 176.7
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.011 220.9
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.012 187.4
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.012 229.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.013 44.2
CdTe (mp-406) <1 1 0> <1 1 0> 0.014 62.5
CdTe (mp-406) <1 1 1> <1 1 1> 0.014 76.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.015 353.4
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.017 76.5
Cu (mp-30) <1 0 0> <1 0 0> 0.022 220.9
LiF (mp-1138) <1 1 0> <1 1 0> 0.023 187.4
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.030 187.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.042 220.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.044 249.9
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.050 309.2
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.050 309.2
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.054 176.7
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.062 124.9
PbSe (mp-2201) <1 0 0> <1 0 0> 0.078 353.4
ZnO (mp-2133) <0 0 1> <1 1 0> 0.087 187.4
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.091 309.2
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.092 353.4
SiC (mp-8062) <1 1 1> <1 1 1> 0.094 229.5
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.100 220.9
GaSb (mp-1156) <1 0 0> <1 0 0> 0.112 353.4
Au (mp-81) <1 0 0> <1 0 0> 0.116 88.3
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.121 124.9
Cu (mp-30) <1 1 0> <1 0 0> 0.122 353.4
Al (mp-134) <1 1 0> <1 1 0> 0.123 187.4
Si (mp-149) <1 1 0> <1 1 0> 0.129 124.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.130 62.5
C (mp-66) <1 0 0> <1 0 0> 0.136 220.9
GaTe (mp-542812) <1 0 0> <1 1 0> 0.137 312.3
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.138 220.9
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.143 187.4
CdSe (mp-2691) <1 0 0> <1 0 0> 0.144 353.4
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
0.55 J/m2 (0.03 eV/Å2)
Weighted work function Φ
4.07 eV
Shape factor η
4.90
Surface energy anisotropy αγ
0.014
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(221) 0.54, 0.03 4.05 0.24
(322) 0.54, 0.03 4.27 0.20
(332) 0.55, 0.03 4.09 0.04
(320) 0.56, 0.03 4.05 0.17
(310) 0.56, 0.03 4.01 0.28
(321) 0.56, 0.03 3.87 0.06
(210) 0.58, 0.04 4.08 0.00
(311) 0.59, 0.04 4.07 0.00
(331) 0.61, 0.04 4.42 0.00
(111) 0.65, 0.04 4.13 0.00
(211) 0.66, 0.04 4.18 0.00
(110) 0.79, 0.05 4.35 0.00
(100) 0.88, 0.06 4.49 0.00

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
59 28 28 0 0 0
28 59 28 0 0 0
28 28 59 0 0 0
0 0 0 26 0 0
0 0 0 0 26 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
24.3 -7.8 -7.8 0 0 0
-7.8 24.3 -7.8 0 0 0
-7.8 -7.8 24.3 0 0 0
0 0 0 38.2 0 0
0 0 0 0 38.2 0
0 0 0 0 0 38.2
Shear Modulus GV
22 GPa
Bulk Modulus KV
38 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
38 GPa
Shear Modulus GVRH
21 GPa
Bulk Modulus KVRH
38 GPa
Elastic Anisotropy
0.33
Poisson's Ratio
0.27

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -4.010 36.868 2.001 7.491
pack_evans_james -4.010 36.871 0.221 3.833
vinet -4.011 36.838 2.046 5.890
tait -4.010 36.840 0.224 5.995
birch_euler -4.010 36.860 0.251 0.857
pourier_tarantola -4.012 36.825 0.039 2.897
birch_lagrange -4.017 36.851 0.147 6.450
murnaghan -4.009 36.915 0.216 3.674
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn3CrS4 (mp-1080726) 0.0175 0.129 3
Zn3CrSe4 (mp-1095028) 0.0124 0.122 3
Zn3CrTe4 (mp-1087545) 0.0105 0.114 3
CdSnSb2 (mp-10063) 0.0250 0.000 3
GaCuS2 (mp-5238) 0.0192 0.000 3
FeCu2GeS4 (mp-917359) 0.0383 0.037 4
CoCu2GeS4 (mp-6498) 0.0382 0.055 4
CoCu2GeS4 (mp-560428) 0.0476 0.055 4
FeCu2GeS4 (mp-22053) 0.0260 0.037 4
FeCu2GeSe4 (mp-1087471) 0.0871 0.037 4
InAs (mp-20305) 0.0000 0.000 2
MoN (mp-13034) 0.0000 0.325 2
HgSe (mp-820) 0.0000 0.000 2
CdTe (mp-406) 0.0000 0.000 2
MnSe (mp-2293) 0.0000 0.004 2
O2 (mp-1057818) 0.0000 1.881 1
Si (mp-149) 0.0000 0.000 1
C (mp-66) 0.0000 0.136 1
Ge (mp-32) 0.0000 0.000 1
Se (mp-12771) 0.0000 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sn_d
Final Energy/Atom
-4.0096 eV
Corrected Energy
-8.0191 eV
Uncorrected energy = -8.0191 eV Corrected energy = -8.0191 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 426976
  • 40039
  • 76040
  • 53789
  • 70128
Submitted by
User remarks:
  • Tin

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)