material

Mg(BeN)2

ID:

mp-11917

DOI:

10.17188/1188466


Tags: Magnesium dinitridodiberyllate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.183 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.03 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.066 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 413358 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.001 204.4
Cu (mp-30) <1 1 1> <0 0 1> 0.004 22.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.006 98.4
YVO4 (mp-19133) <1 0 1> <1 1 0> 0.007 208.9
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.007 52.2
Al (mp-134) <1 0 0> <1 1 0> 0.007 130.6
Au (mp-81) <1 1 1> <1 0 0> 0.007 30.2
Cu (mp-30) <1 0 0> <1 1 0> 0.008 26.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.008 68.1
TiO2 (mp-390) <0 0 1> <1 1 0> 0.008 130.6
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.017 53.0
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.020 130.6
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.022 271.4
C (mp-48) <0 0 1> <0 0 1> 0.022 68.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.026 22.7
Ag (mp-124) <1 1 1> <1 0 0> 0.027 30.2
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.034 185.6
Al (mp-134) <1 1 0> <1 0 1> 0.041 185.6
NaCl (mp-22862) <1 0 0> <1 1 0> 0.042 130.6
GaP (mp-2490) <1 1 1> <0 0 1> 0.047 53.0
GaAs (mp-2534) <1 1 0> <1 0 1> 0.054 185.6
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.060 136.0
ZnSe (mp-1190) <1 0 0> <1 1 0> 0.064 130.6
PbS (mp-21276) <1 1 1> <0 0 1> 0.065 189.2
WS2 (mp-224) <1 1 1> <0 0 1> 0.067 234.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.072 98.4
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.079 185.6
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.079 130.6
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.079 90.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.080 98.4
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.083 130.6
SiC (mp-11714) <1 1 0> <1 0 0> 0.085 271.4
SiC (mp-11714) <1 0 0> <1 1 0> 0.086 156.7
SiC (mp-7631) <1 0 0> <1 1 0> 0.095 235.1
SiC (mp-7631) <1 0 1> <1 0 0> 0.097 286.5
Ag (mp-124) <1 0 0> <1 0 0> 0.097 120.6
SiC (mp-8062) <1 1 1> <0 0 1> 0.098 98.4
GaAs (mp-2534) <1 0 0> <1 1 0> 0.101 130.6
Ge (mp-32) <1 1 0> <1 0 1> 0.107 185.6
DyScO3 (mp-31120) <0 0 1> <1 0 1> 0.108 185.6
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.110 135.0
InP (mp-20351) <1 1 0> <1 0 0> 0.115 150.8
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.116 219.3
PbSe (mp-2201) <1 1 1> <0 0 1> 0.120 68.1
NaCl (mp-22862) <1 1 0> <1 0 1> 0.121 185.6
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.139 211.1
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 1 0> 0.140 104.5
Au (mp-81) <1 0 0> <1 0 0> 0.140 120.6
CaCO3 (mp-3953) <1 0 1> <1 1 0> 0.152 182.8
GaN (mp-804) <1 0 1> <1 0 1> 0.165 135.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
431 64 67 34 0 0
64 431 67 -34 0 0
67 67 407 0 0 0
34 -34 0 154 0 0
0 0 0 0 154 34
0 0 0 0 34 183
Compliance Tensor Sij (10-12Pa-1)
2.5 -0.4 -0.3 -0.6 0 0
-0.4 2.5 -0.3 0.6 0 0
-0.3 -0.3 2.6 0 0 0
-0.6 0.6 0 6.8 0 0
0 0 0 0 6.8 -1.3
0 0 0 0 -1.3 5.7
Shear Modulus GV
169 GPa
Bulk Modulus KV
185 GPa
Shear Modulus GR
163 GPa
Bulk Modulus KR
185 GPa
Shear Modulus GVRH
166 GPa
Bulk Modulus KVRH
185 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.15

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.59 0.00 0.00
0.00 4.59 0.00
0.00 0.00 4.93
Dielectric Tensor εij (total)
11.47 0.00 0.00
0.00 11.47 0.00
0.00 0.00 13.41
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.71
Polycrystalline dielectric constant εpoly
(total)
12.12
Refractive Index n
2.17
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ce2SO2 (mp-3972) 0.0608 0.000 3
U2PN2 (mp-5381) 0.0742 0.000 3
Gd2SO2 (mp-4805) 0.0803 0.000 3
La2SO2 (mp-4511) 0.0729 0.000 3
Pu2SO2 (mp-21421) 0.0491 0.000 3
Li8Mn(O2F)2 (mp-780086) 0.7333 0.071 4
Li6Mn(FeO3)2 (mp-764386) 0.5402 0.040 4
Na2Li3CoO4 (mp-540990) 0.6771 0.075 4
LiCaGaN2 (mp-570948) 0.6430 0.000 4
LiFeCuS2 (mp-755288) 0.4916 0.262 4
Sm2O3 (mp-10733) 0.4133 0.062 2
Pr2O3 (mp-2063) 0.4114 0.026 2
Nd2O3 (mp-2763) 0.4110 0.030 2
Ac2O3 (mp-11107) 0.4140 0.000 2
Th2N3 (mp-1940) 0.3932 0.118 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Be_sv N
Final Energy/Atom
-6.1789 eV
Corrected Energy
-30.8947 eV
-30.8947 eV = -30.8947 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 413358
Submitted by
User remarks:
  • Magnesium dinitridodiberyllate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)