material

PdF4

ID:

mp-13868

DOI:

10.17188/1189787


Tags: Palladium(IV) fluoride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.513 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.670 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fdd2 [43]
Hall
F 2 2d
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 1555 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.003 283.8
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.006 106.0
ZnO (mp-2133) <1 1 1> <0 0 1> 0.018 283.8
GaN (mp-804) <0 0 1> <0 0 1> 0.025 283.8
MgF2 (mp-1249) <1 1 1> <0 1 1> 0.025 242.9
AlN (mp-661) <1 0 1> <1 0 1> 0.027 106.0
Te2Mo (mp-602) <0 0 1> <0 1 0> 0.030 173.2
SiC (mp-7631) <1 0 1> <0 0 1> 0.043 283.8
MgO (mp-1265) <1 0 0> <1 0 0> 0.043 89.5
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.045 106.0
SrTiO3 (mp-4651) <1 0 1> <1 1 0> 0.048 106.5
Bi2Se3 (mp-541837) <0 0 1> <0 1 1> 0.051 242.9
InAs (mp-20305) <1 0 0> <0 0 1> 0.054 113.5
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.055 113.5
InP (mp-20351) <1 0 0> <0 0 1> 0.055 283.8
C (mp-48) <0 0 1> <0 0 1> 0.056 283.8
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.056 81.0
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.057 283.8
CdS (mp-672) <0 0 1> <0 1 1> 0.058 242.9
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.059 106.5
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.060 57.7
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.062 340.6
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.063 340.6
Ag (mp-124) <1 0 0> <0 0 1> 0.065 170.3
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.065 170.3
C (mp-48) <1 0 0> <1 0 0> 0.067 268.6
Ga2O3 (mp-886) <0 1 0> <0 1 0> 0.069 288.7
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.074 227.1
Ag (mp-124) <1 1 0> <0 1 0> 0.075 173.2
CdWO4 (mp-19387) <0 0 1> <0 1 1> 0.075 242.9
CdSe (mp-2691) <1 0 0> <0 0 1> 0.076 113.5
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.076 283.8
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.081 89.5
ZnO (mp-2133) <1 1 0> <0 0 1> 0.082 340.6
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.082 227.1
Au (mp-81) <1 0 0> <0 0 1> 0.083 170.3
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.083 268.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.084 113.5
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.085 340.6
Au (mp-81) <1 1 0> <0 1 0> 0.086 173.2
AlN (mp-661) <1 0 0> <0 0 1> 0.087 283.8
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.091 113.5
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.092 283.8
InSb (mp-20012) <1 0 0> <1 0 0> 0.094 89.5
PbSe (mp-2201) <1 0 0> <0 0 1> 0.096 113.5
WS2 (mp-224) <0 0 1> <1 0 1> 0.097 106.0
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.097 106.0
GaSb (mp-1156) <1 1 0> <0 1 1> 0.100 161.9
PbSe (mp-2201) <1 1 0> <0 1 1> 0.100 161.9
CdSe (mp-2691) <1 1 0> <0 1 1> 0.101 161.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
64 49 21 0 0 0
49 77 30 0 0 0
21 30 31 0 0 0
0 0 0 19 0 0
0 0 0 0 17 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
30.6 -18 -3.7 0 0 0
-18 31.3 -18.1 0 0 0
-3.7 -18.1 52.7 0 0 0
0 0 0 53.3 0 0
0 0 0 0 57.5 0
0 0 0 0 0 26.6
Shear Modulus GV
20 GPa
Bulk Modulus KV
41 GPa
Shear Modulus GR
15 GPa
Bulk Modulus KR
28 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
2.16
Poisson's Ratio
0.29

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.11114 0.00000
0.00000 0.00000 0.00000 0.11132 0.00000 0.00000
0.39022 0.38725 0.42352 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.69398 C/m2
Crystallographic Direction vmax
0.00000
-0.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.26 0.00 -0.00
0.00 6.34 0.00
-0.00 0.00 3.90
Dielectric Tensor εij (total)
7.15 0.00 -0.00
0.00 7.28 0.00
-0.00 0.00 4.22
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.50
Polycrystalline dielectric constant εpoly
(total)
6.22
Refractive Index n
2.34
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AgBi2F12 (mp-28965) 0.4713 0.000 3
Cd(AuF6)2 (mp-557715) 0.3629 0.000 3
Te7(OF5)6 (mp-560802) 0.5586 0.008 3
AgSb2F12 (mp-14653) 0.5255 0.000 3
Au(OF3)2 (mp-3530) 0.5338 0.013 3
Cs2Sb2OF10 (mp-572332) 0.5761 0.003 4
SbBr(OF3)2 (mp-572526) 0.6638 0.000 4
SbI(OF4)2 (mp-557917) 0.4713 0.023 4
Rb3Sc(HO)6 (mp-541483) 0.6557 0.021 4
BaTiOF4 (mp-16915) 0.5975 0.000 4
IrF4 (mp-13841) 0.1944 0.000 2
RuF4 (mp-974434) 0.3443 0.000 2
RhF5 (mp-540622) 0.4509 0.000 2
PtF4 (mp-8943) 0.1282 0.000 2
PtF5 (mp-541341) 0.4291 0.000 2
CuAs2S4(O2F3)4 (mp-556926) 0.7027 0.027 5
CdAs2S2(OF3)4 (mp-558288) 0.6772 0.038 5
MnAs2S2(OF3)4 (mp-562665) 0.7054 0.039 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: F Pd
Final Energy/Atom
-3.6847 eV
Corrected Energy
-36.8469 eV
-36.8469 eV = -36.8469 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 1555
Submitted by
User remarks:
  • Palladium(IV) fluoride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)