Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.245 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnP2 |
Band Gap0.748 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 283.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 264.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 195.6 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 304.7 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 228.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 330.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 167.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 259.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 325.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 228.5 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 188.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 330.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 198.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 304.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 304.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 195.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 152.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 325.9 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 228.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 173.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 278.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 228.5 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 259.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 259.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 259.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 325.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 278.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 223.1 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 152.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 260.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 283.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 330.8 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 111.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 278.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 223.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 260.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 94.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 283.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 228.5 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 228.5 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 278.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 330.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 223.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 167.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 330.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 278.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 65.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 334.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 167.3 |
BN (mp-984) | <1 1 1> | <1 1 0> | 278.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
9.52 | 0.00 | 0.03 |
0.00 | 9.25 | 0.00 |
0.03 | 0.00 | 10.83 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.85 | 0.00 | 0.00 |
0.00 | 10.61 | 0.00 |
0.00 | 0.00 | 12.03 |
Polycrystalline dielectric constant
εpoly∞
9.87
|
Polycrystalline dielectric constant
εpoly
11.16
|
Refractive Index n3.14 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InAgTe2 (mp-675371) | 0.2465 | 0.276 | 3 |
Cu2SnTe3 (mp-675880) | 0.2564 | 0.018 | 3 |
GaAgS2 (mp-556916) | 0.2320 | 0.003 | 3 |
Li2BiO3 (mp-755487) | 0.2641 | 0.093 | 3 |
Zn2ReN3 (mp-1029257) | 0.1867 | 0.000 | 3 |
CdAg2GeS4 (mp-554105) | 0.2685 | 0.003 | 4 |
Cu2HgGeS4 (mp-557574) | 0.3098 | 0.004 | 4 |
Na2CdSnS4 (mp-561075) | 0.3075 | 0.000 | 4 |
MnCu2SiS4 (mp-12023) | 0.2875 | 0.000 | 4 |
CdCu2GeS4 (mp-13982) | 0.3224 | 0.000 | 4 |
ZnAs2 (mp-7262) | 0.2114 | 0.000 | 2 |
ZnP2 (mp-2782) | 0.2361 | 0.000 | 2 |
ZnP2 (mp-680550) | 0.1159 | 0.190 | 2 |
ZnP2 (mp-11025) | 0.2360 | 0.000 | 2 |
CdP2 (mp-402) | 0.3568 | 0.001 | 2 |
Si (mp-971662) | 0.4679 | 0.062 | 1 |
Si (mp-1079297) | 0.3629 | 0.072 | 1 |
C (mp-1078845) | 0.3234 | 0.266 | 1 |
C (mp-1080826) | 0.3448 | 0.299 | 1 |
Si (mp-1095269) | 0.3572 | 0.094 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn P |
Final Energy/Atom-4.2732 eV |
Corrected Energy-102.5567 eV
-102.5567 eV = -102.5567 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)