material

KLaS2

ID:

mp-15781

DOI:

10.17188/1191368


Tags: Potassium lanthanum sulfide Potassium lanthanum disulfide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.244 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.710 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 44942 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 304.1
CdTe (mp-406) <1 1 1> <0 0 1> 0.001 304.1
Ni (mp-23) <1 1 1> <0 0 1> 0.001 64.0
InSb (mp-20012) <1 1 1> <0 0 1> 0.003 304.1
Si (mp-149) <1 1 1> <0 0 1> 0.009 208.1
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.010 112.0
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.011 208.1
GaN (mp-804) <1 0 0> <0 0 1> 0.019 336.1
Ag (mp-124) <1 1 1> <0 0 1> 0.035 208.1
Al (mp-134) <1 1 1> <0 0 1> 0.036 112.0
ZrO2 (mp-2858) <0 0 1> <1 1 0> 0.039 164.5
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.041 224.1
GaP (mp-2490) <1 1 1> <0 0 1> 0.043 208.1
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.047 284.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.050 144.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.060 208.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.061 208.1
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.066 256.1
Ni (mp-23) <1 0 0> <0 0 1> 0.067 256.1
C (mp-48) <0 0 1> <0 0 1> 0.067 16.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.070 128.1
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.081 208.1
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.089 320.1
Au (mp-81) <1 1 1> <0 0 1> 0.091 208.1
AlN (mp-661) <1 1 0> <0 0 1> 0.093 192.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.096 208.1
LaF3 (mp-905) <1 0 0> <0 0 1> 0.097 160.1
LiAlO2 (mp-3427) <1 1 1> <1 1 1> 0.100 165.3
MgO (mp-1265) <1 1 0> <0 0 1> 0.106 128.1
SiC (mp-11714) <1 1 0> <0 0 1> 0.107 272.1
NaCl (mp-22862) <1 1 0> <0 0 1> 0.108 320.1
Mg (mp-153) <1 0 0> <0 0 1> 0.111 336.1
PbS (mp-21276) <1 1 0> <0 0 1> 0.115 256.1
C (mp-48) <1 1 1> <0 0 1> 0.121 240.1
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.123 208.1
AlN (mp-661) <0 0 1> <0 0 1> 0.129 112.0
PbS (mp-21276) <1 0 0> <0 0 1> 0.132 256.1
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.132 192.1
SiC (mp-8062) <1 1 1> <0 0 1> 0.135 304.1
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.138 176.1
TePb (mp-19717) <1 1 1> <0 0 1> 0.150 304.1
WSe2 (mp-1821) <1 1 0> <0 0 1> 0.152 256.1
CdWO4 (mp-19387) <0 1 1> <1 0 1> 0.168 288.9
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.192 192.1
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.194 160.1
Cu (mp-30) <1 1 1> <0 0 1> 0.195 208.1
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.195 272.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.195 189.9
YAlO3 (mp-3792) <1 1 0> <1 1 0> 0.197 164.5
GaN (mp-804) <0 0 1> <0 0 1> 0.201 64.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
79 24 21 5 0 0
24 79 21 -5 0 0
21 21 54 0 0 0
5 -5 0 19 0 0
0 0 0 0 19 5
0 0 0 0 5 27
Compliance Tensor Sij (10-12Pa-1)
15.2 -3.8 -4.3 -4.8 0 0
-3.8 15.2 -4.3 4.8 0 0
-4.3 -4.3 21.8 0 0 0
-4.8 4.8 0 54.3 0 0
0 0 0 0 54.3 -9.5
0 0 0 0 -9.5 38.1
Shear Modulus GV
23 GPa
Bulk Modulus KV
38 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
37 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
37 GPa
Elastic Anisotropy
0.40
Poisson's Ratio
0.25

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.06 0.00 0.00
0.00 5.06 0.00
0.00 0.00 3.81
Dielectric Tensor εij (total)
15.75 0.00 0.00
0.00 15.75 0.00
0.00 0.00 8.25
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.64
Polycrystalline dielectric constant εpoly
(total)
13.25
Refractive Index n
2.15
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaRuO2 (mp-7240) 0.0245 0.079 3
PrSmO2 (mp-867735) 0.0898 0.095 3
NaScO2 (mp-7914) 0.0967 0.000 3
KPrS2 (mp-15782) 0.0921 0.000 3
MgSiN2 (mp-1017514) 0.0530 0.283 3
Li14MgCo13O28 (mp-769537) 0.3041 0.182 4
Li3Al2CrO6 (mp-861573) 0.3121 0.016 4
Li4Co3NiO8 (mp-868138) 0.2965 0.161 4
Li3Fe(CoO3)2 (mp-761602) 0.2866 0.165 4
Li4MgCo3O8 (mp-773461) 0.3140 0.182 4
Sb2Te (mp-6997) 0.3345 0.016 2
Bi2Te3 (mp-568390) 0.3334 0.248 2
TlS (mp-998912) 0.2357 0.062 2
Sb8Te3 (mp-12826) 0.3287 0.003 2
Bi4Te3 (mp-28229) 0.2907 0.000 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.4166 0.005 5
Na (mp-999501) 0.5713 0.114 1
Sb (mp-632286) 0.5336 0.059 1
Bi (mp-23152) 0.5832 0.000 1
Te (mp-570459) 0.5012 0.044 1
Te (mp-105) 0.5929 0.047 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv La S
Final Energy/Atom
-5.4921 eV
Corrected Energy
-23.2952 eV
-23.2952 eV = -21.9683 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 44942
  • 192102
Submitted by
User remarks:
  • Potassium lanthanum sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)