Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.484 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.279 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.6 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 148.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 234.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 234.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 156.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 126.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 234.9 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 234.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 313.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 234.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 313.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 234.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 234.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 313.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 156.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 313.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 126.5 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 234.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 313.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 313.2 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 126.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 156.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 78.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 234.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 156.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 234.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 156.6 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 126.5 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 313.2 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 234.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 156.6 |
Si (mp-149) | <1 1 1> | <0 0 1> | 156.6 |
Au (mp-81) | <1 1 1> | <0 0 1> | 234.9 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 313.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 253.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 156.6 |
CsI (mp-614603) | <1 1 0> | <0 1 0> | 253.0 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 313.2 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 78.3 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 234.9 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 156.6 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 313.2 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 313.2 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 156.6 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 156.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb4SnO3 (mp-769368) | 0.5988 | 0.001 | 3 |
Rb4PbO3 (mp-21801) | 0.2431 | 0.000 | 3 |
LiGdO2 (mp-754162) | 0.6047 | 0.008 | 3 |
K4SnO3 (mp-14988) | 0.3081 | 0.000 | 3 |
BaLi2NiO3 (mp-769677) | 0.5770 | 0.084 | 4 |
MgTaBiO5 (mvc-7416) | 0.5735 | 0.066 | 4 |
MgTiBiO5 (mvc-7422) | 0.5709 | 0.125 | 4 |
ZnCuBiO5 (mvc-7505) | 0.6081 | 0.152 | 4 |
TiZnBiO5 (mvc-7457) | 0.6184 | 0.077 | 4 |
Bi2O3 (mp-37036) | 0.6332 | 0.092 | 2 |
NaLiV(OF)2 (mp-764851) | 0.7145 | 0.078 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Pb_d O |
Final Energy/Atom-4.0952 eV |
Corrected Energy-278.9460 eV
-278.9460 eV = -262.0911 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)