Final Magnetic Moment
1.364 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.122 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.40 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 53459 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.003 192.7
C (mp-48) <1 0 1> <1 1 0> 0.009 139.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.020 139.3
Ni (mp-23) <1 1 1> <0 0 1> 0.020 21.4
GdScO3 (mp-5690) <1 1 1> <1 1 1> 0.037 286.2
Al (mp-134) <1 1 0> <1 1 0> 0.039 69.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.042 139.3
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.045 85.7
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.046 85.7
Au (mp-81) <1 1 0> <1 0 1> 0.046 146.9
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.053 264.4
GaN (mp-804) <1 1 1> <0 0 1> 0.057 214.2
C (mp-48) <1 0 0> <0 0 1> 0.064 192.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.064 313.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.078 278.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.088 69.7
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.090 243.8
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.096 139.3
TbScO3 (mp-31119) <1 1 1> <1 1 1> 0.096 286.2
AlN (mp-661) <1 0 0> <1 0 0> 0.096 140.7
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.097 221.2
Al (mp-134) <1 1 1> <0 0 1> 0.098 85.7
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.099 281.5
Ge (mp-32) <1 1 0> <1 1 0> 0.101 139.3
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.102 104.5
Te2W (mp-22693) <0 0 1> <1 0 0> 0.117 201.1
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.117 221.2
LiF (mp-1138) <1 1 1> <0 0 1> 0.117 85.7
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.118 139.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.118 80.4
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.118 204.4
Te2W (mp-22693) <1 0 1> <1 0 0> 0.133 100.5
Mg (mp-153) <1 1 1> <0 0 1> 0.134 214.2
NaCl (mp-22862) <1 1 0> <1 1 0> 0.142 139.3
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.145 146.9
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.149 140.7
AlN (mp-661) <1 1 0> <1 0 0> 0.154 80.4
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.154 139.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.155 160.9
NaCl (mp-22862) <1 1 1> <1 1 0> 0.157 278.6
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.162 104.5
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.168 321.7
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.170 281.5
DyScO3 (mp-31120) <1 1 1> <1 1 1> 0.177 286.2
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.180 100.5
LiF (mp-1138) <1 1 0> <1 1 0> 0.184 69.7
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.187 85.7
MgO (mp-1265) <1 1 1> <0 0 1> 0.187 278.4
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.195 278.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.198 80.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
269 129 70 0 0 -1
129 269 70 0 0 1
70 70 243 0 0 -0
0 0 0 66 0 0
0 0 0 0 66 0
-1 1 -0 0 0 69
Compliance Tensor Sij (10-12Pa-1)
5 -2.2 -0.8 0 0 0.1
-2.2 5 -0.8 0 0 -0.1
-0.8 -0.8 4.6 0 0 0
0 0 0 15.1 0 0
0 0 0 0 15.1 0
0.1 -0.1 0 0 0 14.5
Shear Modulus GV
74 GPa
Bulk Modulus KV
147 GPa
Shear Modulus GR
72 GPa
Bulk Modulus KR
144 GPa
Shear Modulus GVRH
73 GPa
Bulk Modulus KVRH
145 GPa
Elastic Anisotropy
0.16
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
U2TiH3 (mp-1072971) 0.2186 0.331 3
CoSn (mp-20536) 0.0914 0.000 2
RhPb (mp-442) 0.1898 0.000 2
FeSn (mp-21260) 0.1655 0.000 2
InNi (mp-19876) 0.0940 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Fe_pv Ge_d
Final Energy/Atom
-6.6687 eV
Corrected Energy
-40.0120 eV
Uncorrected energy = -40.0120 eV Corrected energy = -40.0120 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53459
  • 632006
  • 631998
  • 632022
  • 632016
Submitted by
User remarks:
  • Iron germanide (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)