Final Magnetic Moment15.062 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.528 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.793 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 214.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 246.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 134.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 143.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 287.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 287.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 246.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 143.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 287.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 134.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 215.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 215.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 287.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 143.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 287.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 134.2 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 134.2 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 287.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 287.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 -1> | 134.2 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 246.8 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 246.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 234.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 287.3 |
BN (mp-984) | <1 0 0> | <0 1 0> | 214.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 143.7 |
BN (mp-984) | <1 1 0> | <1 0 0> | 234.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 246.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 287.3 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 -1> | 134.2 |
Mg (mp-153) | <1 0 1> | <1 1 1> | 169.7 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 215.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 234.1 |
SiC (mp-7631) | <1 1 1> | <0 1 1> | 246.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 287.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 215.5 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 287.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 143.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 -1> | 134.2 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 287.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 -1> | 134.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 143.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 215.5 |
WSe2 (mp-1821) | <1 0 1> | <0 1 1> | 246.8 |
NaCl (mp-22862) | <1 1 0> | <0 1 -1> | 134.2 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 234.1 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 215.5 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 287.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 215.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg3(AsO4)2 (mp-756919) | 0.4567 | 0.000 | 3 |
Co3(AsO4)2 (mp-25740) | 0.4960 | 0.476 | 3 |
Mg3(PO4)2 (mp-14396) | 0.4326 | 0.000 | 3 |
Co3(PO4)2 (mp-19264) | 0.4588 | 0.000 | 3 |
Co3(PO4)2 (mp-608109) | 0.4439 | 0.000 | 3 |
Li3Ti3(PO4)4 (mp-758035) | 0.1849 | 0.079 | 4 |
Li3Fe3(PO4)4 (mp-31842) | 0.1470 | 0.009 | 4 |
Li3V3(PO4)4 (mp-32511) | 0.1800 | 0.015 | 4 |
Li3V3(PO4)4 (mp-32528) | 0.1263 | 0.002 | 4 |
Li3V3(PO4)4 (mp-705268) | 0.1277 | 0.002 | 4 |
Li2V2SiGeO10 (mp-767479) | 0.7086 | 0.060 | 5 |
FeCoPO4F (mp-705338) | 0.6277 | 0.006 | 5 |
Li2V2SiGeO10 (mp-765775) | 0.7019 | 0.061 | 5 |
LiCrPO4F (mp-762791) | 0.5629 | 0.204 | 5 |
Y4Ti13Si2(SbO14)2 (mvc-9261) | 0.6574 | 0.413 | 5 |
Li3MnVP2(O4F)2 (mp-763904) | 0.7453 | 0.034 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.8559 eV |
Corrected Energy-593.0666 eV
-593.0666 eV = -534.7596 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 24.5970 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)