material

YSiPd2

ID:

mp-28024

DOI:

10.17188/1202159


Tags: Yttrium palladium silicide (1/2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.985 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.66 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 35087 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2W (mp-22693) <0 1 1> <0 0 1> 0.017 116.4
TiO2 (mp-2657) <1 1 1> <0 1 0> 0.017 204.0
Te2W (mp-22693) <0 1 0> <1 0 1> 0.019 323.0
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.022 163.2
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.023 326.3
ZnO (mp-2133) <1 0 1> <1 0 0> 0.024 258.2
CaF2 (mp-2741) <1 0 0> <0 1 0> 0.024 122.4
Mg (mp-153) <1 1 0> <0 0 1> 0.024 116.4
BaTiO3 (mp-5986) <1 0 0> <0 1 1> 0.024 168.9
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.031 155.2
GaN (mp-804) <1 1 0> <0 0 1> 0.034 116.4
Al (mp-134) <1 1 0> <1 0 0> 0.040 206.6
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.049 77.6
Mg (mp-153) <0 0 1> <0 1 0> 0.051 122.4
GaN (mp-804) <1 1 1> <0 1 0> 0.054 122.4
YAlO3 (mp-3792) <0 1 1> <1 0 1> 0.061 193.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.061 310.5
GaP (mp-2490) <1 0 0> <0 1 0> 0.062 122.4
MoSe2 (mp-1634) <1 0 0> <1 0 1> 0.064 258.4
CsI (mp-614603) <1 0 0> <0 0 1> 0.083 310.5
InP (mp-20351) <1 1 1> <1 0 0> 0.084 309.9
PbS (mp-21276) <1 1 1> <1 0 0> 0.091 309.9
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.095 122.4
WS2 (mp-224) <0 0 1> <0 1 0> 0.096 122.4
Mg (mp-153) <1 1 1> <0 1 0> 0.100 122.4
TbScO3 (mp-31119) <0 1 1> <0 1 0> 0.100 163.2
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.104 154.9
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.119 129.2
Fe2O3 (mp-24972) <1 0 0> <0 1 1> 0.119 281.5
MgF2 (mp-1249) <0 0 1> <0 1 0> 0.126 326.3
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.134 194.0
TeO2 (mp-2125) <0 1 1> <0 1 1> 0.135 225.2
SrTiO3 (mp-4651) <0 0 1> <0 1 0> 0.136 122.4
TeO2 (mp-2125) <0 1 0> <0 1 0> 0.137 204.0
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.138 310.5
LiGaO2 (mp-5854) <0 0 1> <0 1 1> 0.140 56.3
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.142 131.6
TiO2 (mp-2657) <1 0 0> <1 0 1> 0.145 193.8
CdS (mp-672) <0 0 1> <0 1 0> 0.149 122.4
LiGaO2 (mp-5854) <1 0 1> <0 1 1> 0.158 225.2
Ni (mp-23) <1 1 1> <0 0 1> 0.163 194.0
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.164 122.4
BN (mp-984) <1 0 1> <1 1 1> 0.178 305.6
Cu (mp-30) <1 0 0> <0 1 1> 0.184 225.2
SrTiO3 (mp-4651) <1 0 1> <0 1 0> 0.185 163.2
PbSe (mp-2201) <1 1 0> <1 1 0> 0.196 329.1
WS2 (mp-224) <1 1 0> <0 0 1> 0.198 77.6
DyScO3 (mp-31120) <0 1 1> <0 1 0> 0.198 163.2
CeO2 (mp-20194) <1 1 0> <0 1 1> 0.201 168.9
GaSb (mp-1156) <1 1 0> <1 1 0> 0.201 329.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
224 101 83 0 0 0
101 182 93 0 0 0
83 93 182 0 0 0
0 0 0 58 0 0
0 0 0 0 41 0
0 0 0 0 0 51
Compliance Tensor Sij (10-12Pa-1)
6.2 -2.7 -1.5 0 0 0
-2.7 8.6 -3.2 0 0 0
-1.5 -3.2 7.8 0 0 0
0 0 0 17.2 0 0
0 0 0 0 24.5 0
0 0 0 0 0 19.8
Shear Modulus GV
51 GPa
Bulk Modulus KV
127 GPa
Shear Modulus GR
49 GPa
Bulk Modulus KR
126 GPa
Shear Modulus GVRH
50 GPa
Bulk Modulus KVRH
126 GPa
Elastic Anisotropy
0.14
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeGaPd2 (mp-639863) 0.2809 0.000 3
MgNi2P (mp-17942) 0.2430 0.000 3
YbSiPt2 (mp-864645) 0.2088 0.000 3
ErSiPd2 (mp-3352) 0.0948 0.000 3
ErGePd2 (mp-20819) 0.2709 0.000 3
TbH3 (mp-982384) 0.5906 0.000 2
YH3 (mp-23706) 0.5671 0.000 2
NdH3 (mp-976578) 0.6028 0.000 2
MgSi (mp-1073754) 0.5881 0.195 2
GdH3 (mp-505686) 0.5944 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Si Pd
Final Energy/Atom
-6.5469 eV
Corrected Energy
-104.7510 eV
-104.7510 eV = -104.7510 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 35087
Submitted by
User remarks:
  • Yttrium palladium silicide (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)