Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.248 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2NF |
Band Gap1.720 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 289.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 193.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 290.3 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 228.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 283.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 283.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 290.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 193.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 144.7 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 152.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 217.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 145.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 217.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 217.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 228.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 217.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 204.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 217.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 169.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 217.1 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 217.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 217.8 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 283.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 338.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 153.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 153.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 314.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 339.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 121.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 266.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 121.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 266.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 314.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 283.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 217.8 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 204.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 217.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 204.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 145.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 121.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 169.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 193.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 121.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
153 | 56 | 42 | 0 | 0 | 0 |
56 | 153 | 42 | -0 | 0 | 0 |
42 | 42 | 69 | -0 | 0 | 0 |
0 | -0 | -0 | 52 | 0 | 0 |
0 | 0 | 0 | 0 | 52 | 0 |
0 | 0 | 0 | 0 | 0 | 60 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.3 | -2 | -3.9 | 0 | 0 | 0 |
-2 | 8.3 | -3.9 | 0 | 0 | 0 |
-3.9 | -3.9 | 19.3 | 0 | 0 | 0 |
0 | 0 | 0 | 19.2 | 0 | 0 |
0 | 0 | 0 | 0 | 19.2 | 0 |
0 | 0 | 0 | 0 | 0 | 16.8 |
Shear Modulus GV48 GPa |
Bulk Modulus KV73 GPa |
Shear Modulus GR43 GPa |
Bulk Modulus KR61 GPa |
Shear Modulus GVRH46 GPa |
Bulk Modulus KVRH67 GPa |
Elastic Anisotropy0.82 |
Poisson's Ratio0.22 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.57 | -0.00 | 0.20 |
-0.00 | 4.43 | 0.00 |
0.20 | 0.00 | 4.73 |
Dielectric Tensor εij (total) |
||
---|---|---|
17.92 | -0.00 | 2.75 |
-0.00 | 16.08 | -0.00 |
2.75 | -0.00 | 20.19 |
Polycrystalline dielectric constant
εpoly∞
4.58
|
Polycrystalline dielectric constant
εpoly
18.06
|
Refractive Index n2.14 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaAsSe2 (mp-34663) | 0.1463 | 0.115 | 3 |
LiCrO2 (mp-762454) | 0.1125 | 0.038 | 3 |
KBiSe2 (mp-36539) | 0.0920 | 0.054 | 3 |
NaYbO2 (mp-756878) | 0.0398 | 0.098 | 3 |
LiNiO2 (mp-770635) | 0.0673 | 0.015 | 3 |
Li2CrFeO4 (mp-771605) | 0.1231 | 1.035 | 4 |
Li2CoCuO4 (mp-775052) | 0.0969 | 0.090 | 4 |
Li2MnCrO4 (mp-773308) | 0.0933 | 0.035 | 4 |
Li2CrNiO4 (mp-773255) | 0.1382 | 0.073 | 4 |
Li2CoNiO4 (mp-761608) | 0.1580 | 0.088 | 4 |
Te2Au (mp-1662) | 0.5673 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3965 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.5496 | 0.009 | 2 |
BaO (mp-776658) | 0.6575 | 0.019 | 2 |
Te2Au (mp-567525) | 0.5237 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6213 | 0.005 | 5 |
Sb (mp-632286) | 0.7052 | 0.059 | 1 |
Te (mp-570459) | 0.6546 | 0.044 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv N F |
Final Energy/Atom-5.5942 eV |
Corrected Energy-44.7538 eV
-44.7538 eV = -44.7538 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)