material

TiO2

ID:

mp-34688

DOI:

10.17188/1206871

Warnings: [?]
  1. Large change in a lattice parameter during relaxation.
  2. Large change in volume during relaxation.

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.509 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.015 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.80 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiO2
Band Gap
1.998 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/c [15]
Hall
-C 2yc
Point Group
2/m
Crystal System
monoclinic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.003 263.3
LaAlO3 (mp-2920) <1 1 1> <1 0 1> 0.012 252.0
Al (mp-134) <1 0 0> <0 0 1> 0.012 146.3
MoS2 (mp-1434) <1 1 1> <1 1 -1> 0.015 118.7
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.018 146.3
GaAs (mp-2534) <1 0 0> <0 0 1> 0.018 263.3
TePb (mp-19717) <1 0 0> <0 1 0> 0.023 128.9
Cu (mp-30) <1 0 0> <0 0 1> 0.029 117.0
LiAlO2 (mp-3427) <1 0 0> <1 0 -1> 0.032 330.0
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 0.042 50.4
C (mp-48) <0 0 1> <1 0 1> 0.045 100.8
CdTe (mp-406) <1 1 1> <1 0 1> 0.047 151.2
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.050 128.9
WS2 (mp-224) <1 1 0> <1 1 -1> 0.050 79.1
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.055 263.3
InSb (mp-20012) <1 1 1> <1 0 1> 0.062 151.2
GdScO3 (mp-5690) <1 0 1> <0 1 0> 0.068 335.3
Ge (mp-32) <1 0 0> <0 0 1> 0.070 263.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.074 146.3
AlN (mp-661) <0 0 1> <1 0 1> 0.077 50.4
TeO2 (mp-2125) <0 1 0> <0 1 0> 0.079 206.3
TiO2 (mp-390) <0 0 1> <0 0 1> 0.083 29.3
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.089 302.4
TbScO3 (mp-31119) <0 0 1> <1 1 -1> 0.092 158.2
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.092 175.6
NdGaO3 (mp-3196) <0 1 1> <1 1 -1> 0.102 158.2
ZnO (mp-2133) <1 1 1> <1 1 0> 0.114 156.4
TeO2 (mp-2125) <0 1 1> <1 0 -1> 0.115 150.0
SiC (mp-8062) <1 1 1> <1 0 1> 0.118 100.8
BaF2 (mp-1029) <1 1 0> <1 1 -1> 0.119 276.9
ZrO2 (mp-2858) <0 1 0> <1 1 -1> 0.121 197.8
SiC (mp-11714) <1 1 0> <1 0 -1> 0.126 270.0
TiO2 (mp-390) <1 0 1> <0 0 1> 0.127 321.8
SiC (mp-7631) <1 0 0> <0 0 1> 0.133 234.1
TePb (mp-19717) <1 1 1> <1 0 1> 0.136 151.2
SiC (mp-7631) <0 0 1> <1 0 1> 0.142 50.4
TiO2 (mp-2657) <1 1 0> <1 0 -1> 0.147 270.0
PbSe (mp-2201) <1 1 0> <1 1 -1> 0.148 276.9
CdWO4 (mp-19387) <0 1 0> <1 0 -1> 0.150 240.0
SiC (mp-11714) <0 0 1> <1 0 1> 0.154 50.4
GdScO3 (mp-5690) <0 0 1> <1 1 -1> 0.155 158.2
MgF2 (mp-1249) <1 0 1> <1 1 -1> 0.160 79.1
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.166 87.8
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.173 263.3
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.180 87.8
SiC (mp-11714) <1 1 1> <0 1 1> 0.180 273.0
PbS (mp-21276) <1 0 0> <0 0 1> 0.185 146.3
CdWO4 (mp-19387) <0 0 1> <0 1 1> 0.187 273.0
GaSb (mp-1156) <1 1 0> <1 1 -1> 0.190 276.9
GaSe (mp-1943) <0 0 1> <0 0 1> 0.202 204.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
328 147 141 0 0 -0
147 328 141 0 0 -0
141 141 191 0 0 -0
0 0 0 48 0 0
0 0 0 0 48 0
-0 -0 -0 0 0 58
Compliance Tensor Sij (10-12Pa-1)
4.6 -0.9 -2.8 0 0 0
-0.9 4.6 -2.8 0 0 0
-2.8 -2.8 9.3 0 0 0
0 0 0 21 -0.1 0
0 0 0 -0.1 21 0
0 0 0 0 0 17.1
Shear Modulus GV
59 GPa
Bulk Modulus KV
190 GPa
Shear Modulus GR
54 GPa
Bulk Modulus KR
174 GPa
Shear Modulus GVRH
56 GPa
Bulk Modulus KVRH
182 GPa
Elastic Anisotropy
0.51
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiNbO4 (mp-755302) 0.1133 0.042 3
TiVO4 (mp-780818) 0.1267 0.095 3
TiFeO4 (mp-773534) 0.1142 0.087 3
CrSbO4 (mp-774153) 0.1394 0.067 3
MnSbO4 (mp-774143) 0.1398 0.052 3
LiFe5(OF2)4 (mp-782691) 0.3847 0.067 4
CaNiWO6 (mvc-14986) 0.5117 0.286 4
Ti2Mn3Cr3O16 (mp-771540) 0.5427 0.075 4
Mn3Cr3(WO8)2 (mp-778921) 0.5508 0.084 4
LiV(OF)2 (mp-764229) 0.4658 0.027 4
FeO2 (mp-715178) 0.1477 0.144 2
IrO2 (mp-1014261) 0.1172 0.258 2
SnO2 (mp-755071) 0.2219 0.057 2
TiO2 (mp-390) 0.1498 0.006 2
CeSe2 (mp-1080295) 0.1392 0.120 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Mesoporous TiO2 photocatalysts have been synthesized using polyethylene glycol (PEG) as a template direction agent in diluted acetic acid aqueous solution. This medium slows down the hydrolysis reacti [...]
Aluminum pillared clay (Al-PILC) and platinum impregnated pillared clay (Pt/Al-PILC) were prepared, characterized and tested as catalysts in adipic ester hydrogenation. Results were compared with thos [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition TiO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv O
Final Energy/Atom
-8.9585 eV
Corrected Energy
-56.5601 eV
-56.5601 eV = -53.7510 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • Ordering of Disordered Crystal

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)