Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.485 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 235.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 235.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 142.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 294.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 192.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 176.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 235.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 142.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 294.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 235.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 294.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 259.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 294.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 142.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 294.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 259.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 235.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 142.3 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 142.7 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 294.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 176.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 294.5 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 235.6 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 235.6 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 235.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 235.6 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 235.6 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 294.5 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 0> | 259.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 117.8 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 192.7 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 117.8 |
YAlO3 (mp-3792) | <1 0 1> | <1 1 0> | 192.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 129.5 |
CsI (mp-614603) | <1 1 0> | <0 0 1> | 176.7 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 192.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 176.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 294.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 294.5 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 176.7 |
SrTiO3 (mp-4651) | <1 1 1> | <1 0 0> | 142.7 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 235.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 235.6 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 142.7 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 294.5 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 1> | 142.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 294.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 176.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 142.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 192.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn(PO3)2 (mp-767141) | 0.2836 | 0.003 | 3 |
Ca(PO3)2 (mp-5680) | 0.1397 | 0.000 | 3 |
P2PbO6 (mp-3476) | 0.2537 | 0.000 | 3 |
Lu2P4O13 (mp-773016) | 0.5365 | 0.063 | 3 |
Nd6Mo10O39 (mp-578718) | 0.5362 | 0.006 | 3 |
KCe(PO3)4 (mp-977037) | 0.5520 | 0.005 | 4 |
CsNd(PO3)4 (mp-17605) | 0.5600 | 0.004 | 4 |
CsPr(PO3)4 (mp-17770) | 0.5383 | 0.000 | 4 |
KBa2(PO3)5 (mp-560320) | 0.5442 | 0.000 | 4 |
CsTb(PO3)4 (mp-17128) | 0.5877 | 0.000 | 4 |
CsUGa(PO5)2 (mp-559852) | 0.7008 | 0.000 | 5 |
RbPrP3HO10 (mp-601292) | 0.6626 | 0.035 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv P O |
Final Energy/Atom-7.2253 eV |
Corrected Energy-553.9344 eV
-553.9344 eV = -520.2245 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)