Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.450 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.578 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 16892 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Cu (mp-30) <1 1 1> <0 0 1> 0.000 90.7
Au (mp-81) <1 1 1> <0 0 1> 0.001 30.2
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.002 211.6
YVO4 (mp-19133) <1 1 0> <1 1 0> 0.003 194.6
KCl (mp-23193) <1 1 1> <0 0 1> 0.004 211.6
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.005 308.9
ZnO (mp-2133) <1 1 1> <1 1 1> 0.008 286.3
SiC (mp-8062) <1 0 0> <1 0 1> 0.009 288.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.009 211.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.009 120.9
LiGaO2 (mp-5854) <0 1 1> <1 1 1> 0.009 171.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.010 120.9
Mg (mp-153) <1 0 1> <1 0 0> 0.010 56.2
BN (mp-984) <0 0 1> <1 1 1> 0.011 114.5
Ag (mp-124) <1 1 1> <0 0 1> 0.011 30.2
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.012 243.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.012 90.7
Te2W (mp-22693) <1 0 0> <1 0 0> 0.013 196.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.013 362.7
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.014 308.9
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.017 308.9
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.021 243.2
InP (mp-20351) <1 0 0> <1 0 0> 0.022 140.4
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.022 308.9
CdS (mp-672) <1 0 1> <1 0 0> 0.025 196.6
Ni (mp-23) <1 1 0> <1 0 1> 0.027 206.3
AlN (mp-661) <1 0 1> <1 0 0> 0.028 252.7
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.028 145.9
C (mp-48) <0 0 1> <1 0 1> 0.028 165.0
Al (mp-134) <1 1 1> <0 0 1> 0.028 362.7
Cu (mp-30) <1 0 0> <0 0 1> 0.029 211.6
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.029 196.6
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.030 280.8
C (mp-66) <1 1 0> <1 1 0> 0.032 145.9
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.032 286.3
Cu (mp-30) <1 1 0> <1 1 0> 0.037 145.9
C (mp-48) <1 0 0> <0 0 1> 0.038 362.7
Ge (mp-32) <1 1 1> <1 0 1> 0.038 288.8
Au (mp-81) <1 0 0> <1 0 1> 0.039 123.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.039 211.6
AlN (mp-661) <1 1 1> <1 1 0> 0.041 340.5
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.043 196.6
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.047 196.6
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.049 224.7
C (mp-48) <1 1 0> <1 0 0> 0.049 196.6
GaAs (mp-2534) <1 1 1> <1 0 1> 0.051 288.8
Ga2O3 (mp-886) <0 1 0> <1 0 0> 0.052 140.4
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.053 112.3
GaN (mp-804) <1 0 1> <1 0 0> 0.057 56.2
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.057 308.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
51 19 16 4 0 0
19 51 16 -4 0 0
16 16 36 0 0 0
4 -4 0 6 0 0
0 0 0 0 6 4
0 0 0 0 4 16
Compliance Tensor Sij (10-12Pa-1)
27.5 -9.4 -8.1 -21.2 0 0
-9.4 27.5 -8.1 21.2 0 0
-8.1 -8.1 35 0 0 0
-21.2 21.2 0 181.4 0 0
0 0 0 0 181.4 -42.3
0 0 0 0 -42.3 73.8
Shear Modulus GV
11 GPa
Bulk Modulus KV
27 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
26 GPa
Shear Modulus GVRH
10 GPa
Bulk Modulus KVRH
26 GPa
Elastic Anisotropy
1.76
Poisson's Ratio
0.33

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.40 0.00 0.00
0.00 2.40 0.00
0.00 0.00 2.26
Dielectric Tensor εij (total)
7.49 0.00 -0.00
0.00 7.49 -0.00
-0.00 -0.00 8.70
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.35
Polycrystalline dielectric constant εpoly
(total)
7.89
Refractive Index n
1.53
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Rb2PtF6 (mp-8192) 0.1724 0.000 3
K2RhF6 (mp-8018) 0.1207 0.000 3
K2PdF6 (mp-7979) 0.1094 0.000 3
K2ReF6 (mp-7824) 0.1983 0.000 3
K2IrF6 (mp-11174) 0.0895 0.000 3
Cs4TlSbCl12 (mp-650007) 0.5349 0.000 4
Cs2TlSiH6 (mp-989560) 0.6665 0.013 4
Cs2SeClF6 (mp-989544) 0.6696 0.000 4
Cs4BiSbCl12 (mp-23583) 0.5797 0.000 4
LiMgH6Ir (mp-866640) 0.5249 0.000 4
Rb19O3 (mp-779582) 0.7083 0.047 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv Pt F
Final Energy/Atom
-4.3170 eV
Corrected Energy
-38.8533 eV
-38.8533 eV = -38.8533 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 16892
  • 87360
Submitted by
User remarks:
  • Potassium hexafluoroplatinate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)