Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.846 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.32 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NaNbO3
Band Gap
2.788 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [161]
Hall
R 3 2"c
Point Group
3m
Crystal System
trigonal
We have not yet calculated a detailed bandstructure for this material

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
DyScO3 (mp-31120) <0 1 0> <1 0 0> 313.0
DyScO3 (mp-31120) <0 1 1> <0 0 1> 53.8
DyScO3 (mp-31120) <1 1 0> <1 0 0> 313.0
ZnSe (mp-1190) <1 1 1> <1 0 0> 234.7
KTaO3 (mp-3614) <1 0 0> <0 0 1> 80.7
KTaO3 (mp-3614) <1 1 0> <0 0 1> 161.4
KTaO3 (mp-3614) <1 1 1> <0 0 1> 26.9
CdS (mp-672) <0 0 1> <0 0 1> 107.6
CdS (mp-672) <1 0 0> <1 0 0> 234.7
LiF (mp-1138) <1 0 0> <0 0 1> 296.0
LiF (mp-1138) <1 1 1> <0 0 1> 349.8
Te2W (mp-22693) <0 1 1> <1 0 0> 234.7
YVO4 (mp-19133) <1 0 0> <0 0 1> 188.3
YVO4 (mp-19133) <1 0 1> <1 1 0> 135.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 349.8
Ag (mp-124) <1 1 1> <0 0 1> 349.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 322.9
GaSe (mp-1943) <0 0 1> <0 0 1> 242.2
BN (mp-984) <0 0 1> <0 0 1> 296.0
BN (mp-984) <1 0 0> <0 0 1> 349.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 322.9
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 26.9
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 215.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 107.6
AlN (mp-661) <0 0 1> <0 0 1> 107.6
AlN (mp-661) <1 0 1> <0 0 1> 322.9
AlN (mp-661) <1 1 1> <1 0 0> 234.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 26.9
MoS2 (mp-1434) <1 1 0> <1 0 0> 234.7
MoS2 (mp-1434) <1 1 1> <1 0 0> 234.7
Al (mp-134) <1 0 0> <0 0 1> 80.7
Al (mp-134) <1 1 0> <0 0 1> 161.4
Al (mp-134) <1 1 1> <0 0 1> 26.9
CeO2 (mp-20194) <1 0 0> <0 0 1> 215.3
CeO2 (mp-20194) <1 1 0> <0 0 1> 215.3
GaAs (mp-2534) <1 1 1> <1 0 0> 234.7
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 313.0
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 107.6
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 234.7
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 188.3
GaN (mp-804) <0 0 1> <0 0 1> 26.9
GaN (mp-804) <1 0 0> <1 0 0> 234.7
GaN (mp-804) <1 1 0> <1 0 0> 234.7
GaN (mp-804) <1 1 1> <1 0 0> 156.5
CdTe (mp-406) <1 0 0> <0 0 1> 134.5
CdTe (mp-406) <1 1 0> <0 0 1> 322.9
CdTe (mp-406) <1 1 1> <0 0 1> 80.7
SiO2 (mp-6930) <0 0 1> <0 0 1> 188.3
SiO2 (mp-6930) <1 0 0> <1 0 0> 313.0
TeO2 (mp-2125) <0 0 1> <1 0 0> 156.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
189 69 60 19 0 0
69 189 60 -19 0 0
60 60 174 0 0 0
19 -19 0 37 0 0
0 0 0 0 37 19
0 0 0 0 19 60
Compliance Tensor Sij (10-12Pa-1)
7.3 -2.7 -1.6 -5.2 0 0
-2.7 7.3 -1.6 5.2 0 0
-1.6 -1.6 6.9 0 0 0
-5.2 5.2 0 32.6 0 0
0 0 0 0 32.6 -10.4
0 0 0 0 -10.4 20.1
Shear Modulus GV
51 GPa
Bulk Modulus KV
103 GPa
Shear Modulus GR
41 GPa
Bulk Modulus KR
103 GPa
Shear Modulus GVRH
46 GPa
Bulk Modulus KVRH
103 GPa
Elastic Anisotropy
1.18
Poisson's Ratio
0.31

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -4.34151 2.70347
2.70347 -2.70347 0.00000 -4.34151 0.00000 0.00000
-0.80325 -0.80325 -2.91139 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
5.78500 C/m2
Crystallographic Direction vmax
0.00000
1.00000
-0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.47 -0.00 0.00
-0.00 5.47 -0.00
0.00 -0.00 4.99
Dielectric Tensor εij (total)
43.47 -0.00 -0.00
-0.00 43.47 -0.00
-0.00 -0.00 26.76
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.31
Polycrystalline dielectric constant εpoly
(total)
37.90
Refractive Index n
2.31
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
RbSnCl3 (mp-998611) 0.3438 0.000 3
YWN3 (mp-989576) 0.3693 0.046 3
LaMoN3 (mp-989552) 0.4175 0.029 3
LaWN3 (mp-989524) 0.3124 0.000 3
GaBiO3 (mp-755568) 0.4061 0.051 3
NaTi2BiO6 (mp-39681) 0.2594 0.014 4
Ca2MnWO6 (mvc-16535) 0.4699 0.021 4
TiFe(BiO3)2 (mp-560185) 0.5089 0.015 4
Ca2CoWO6 (mvc-16560) 0.4689 0.025 4
Ca2FeWO6 (mvc-12913) 0.4938 0.022 4
FeSb3 (mp-971669) 0.7128 0.000 2
Zn3N2 (mp-9460) 0.7102 0.000 2
LuO3 (mp-1021512) 0.7420 0.662 2
CoSb3 (mp-1317) 0.7330 0.000 2
SrCoBiRuO6 (mp-743579) 0.6177 0.171 5
BaNdNiSbO6 (mp-41829) 0.6213 0.118 5
LaMgFeCuO6 (mvc-8936) 0.6279 0.092 5
LaZnFeCuO6 (mvc-9037) 0.6135 0.292 5
BaNdNiSbO6 (mp-705415) 0.6179 0.118 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

NaNbO3 was synthesized by two different routes, one using metallic niobium powder, and another using niobium oxide (Nb2O5) powder. In both routes an aqueous sodium hydroxide solution was used to hydro [...]
A solid-state reaction method was used to prepare the BaTiO3Bi(Zn1/2Ti1/2)O3NaNbO3 solid solutions from BaCO3 (99.8%), Bi2O3 (99.9%), Na2CO3 (99.5%), ZnO (99.9%), Nb2O5 (99.9%), and TiO2 (99.0 [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition NaNbO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Nb_pv O
Final Energy/Atom
-7.6760 eV
Corrected Energy
-80.9737 eV
-80.9737 eV = -76.7599 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 252479
  • 28152
  • 9645
Submitted by
User remarks:
  • Sodium niobate(V) - LT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)