Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.989 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaSbS2 |
Band Gap0.954 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 228.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 228.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 229.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.2 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 228.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 298.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 129.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 91.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 91.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 64.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 71.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 132.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 143.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 298.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 166.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 274.1 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 283.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 99.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 265.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 132.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 91.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 64.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 166.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 91.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 166.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 199.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 -1> | 283.7 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 298.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 64.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 64.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 166.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 332.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 298.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 66.4 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 228.8 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 99.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 99.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 232.4 |
YVO4 (mp-19133) | <1 0 1> | <1 1 -1> | 283.7 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 182.8 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 229.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 228.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 274.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 259.2 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 228.8 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 274.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 99.6 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 298.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 206.6 |
BN (mp-984) | <1 1 0> | <1 1 0> | 305.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3TaO4 (mp-3151) | 0.4278 | 0.000 | 3 |
Li2BiO3 (mp-769026) | 0.4138 | 0.051 | 3 |
Li4MoO5 (mp-699343) | 0.3352 | 0.026 | 3 |
Li2TeSe3 (mp-570080) | 0.4052 | 0.000 | 3 |
Na4UO5 (mp-5327) | 0.4310 | 0.000 | 3 |
Li3VSiO5 (mp-861563) | 0.3429 | 0.147 | 4 |
Li2VO2F (mp-764822) | 0.3347 | 0.099 | 4 |
Li5V3(NiO5)2 (mp-851083) | 0.3308 | 0.139 | 4 |
Li5Mn3(NiO5)2 (mp-773349) | 0.3588 | 0.075 | 4 |
Li2TiFe2O5 (mp-769668) | 0.3315 | 0.515 | 4 |
FeO (mp-849689) | 0.6957 | 0.104 | 2 |
NaTe3 (mp-28478) | 0.5964 | 0.000 | 2 |
Te2Au (mp-571547) | 0.5739 | 0.010 | 2 |
BaO (mp-776658) | 0.6008 | 0.019 | 2 |
Te2Au (mp-567525) | 0.5908 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6959 | 0.005 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Sb S |
Final Energy/Atom-4.0863 eV |
Corrected Energy-35.3440 eV
-35.3440 eV = -32.6902 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)