material

Y2Si2O7

ID:

mp-5652

DOI:

10.17188/1272413


Tags: Diyttrium disilicate - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.676 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.013 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Y2Si2O7
Band Gap
4.804 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 281312 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.015 315.1
KCl (mp-23193) <1 1 0> <1 0 0> 0.017 174.1
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.028 189.1
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.028 261.2
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.042 189.1
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.048 217.3
ZrO2 (mp-2858) <1 0 0> <1 1 -1> 0.050 228.3
LiTaO3 (mp-3666) <1 1 0> <0 0 1> 0.051 126.1
CdS (mp-672) <0 0 1> <0 1 0> 0.059 259.9
LiF (mp-1138) <1 0 0> <1 0 1> 0.069 83.7
C (mp-48) <1 1 1> <1 1 -1> 0.071 304.4
C (mp-48) <0 0 1> <1 1 0> 0.079 217.3
Au (mp-81) <1 1 0> <1 1 0> 0.096 271.6
CdWO4 (mp-19387) <0 0 1> <0 1 1> 0.098 212.7
C (mp-66) <1 0 0> <1 0 1> 0.103 167.3
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.103 130.6
Ge (mp-32) <1 0 0> <1 0 1> 0.107 167.3
GdScO3 (mp-5690) <1 0 1> <1 1 -1> 0.112 228.3
SiC (mp-7631) <1 1 1> <0 1 0> 0.123 162.4
WS2 (mp-224) <0 0 1> <1 0 0> 0.125 348.3
GaN (mp-804) <1 1 0> <0 1 0> 0.125 259.9
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.126 348.3
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.129 259.9
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.129 259.9
Ag (mp-124) <1 1 0> <1 1 0> 0.143 271.6
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.144 217.7
AlN (mp-661) <0 0 1> <0 1 0> 0.149 227.4
Cu (mp-30) <1 0 0> <1 0 -1> 0.151 275.3
DyScO3 (mp-31120) <0 0 1> <0 1 1> 0.154 283.6
TiO2 (mp-390) <1 1 0> <1 0 0> 0.159 261.2
YAlO3 (mp-3792) <0 0 1> <1 1 -1> 0.160 228.3
Ga2O3 (mp-886) <1 0 1> <1 0 -1> 0.163 137.6
GaN (mp-804) <1 0 0> <1 1 0> 0.166 217.3
LiTaO3 (mp-3666) <1 0 1> <1 0 0> 0.166 304.7
Mg (mp-153) <1 1 0> <1 1 -1> 0.166 228.3
GaAs (mp-2534) <1 0 0> <1 0 1> 0.169 167.3
YAlO3 (mp-3792) <0 1 0> <1 0 -1> 0.169 275.3
TbScO3 (mp-31119) <0 0 1> <0 1 1> 0.176 283.6
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.176 325.9
CdS (mp-672) <1 1 0> <0 0 1> 0.183 252.1
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.186 189.1
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.198 325.9
SiO2 (mp-6930) <1 1 0> <0 1 1> 0.201 141.8
BaTiO3 (mp-5986) <1 1 1> <1 1 -1> 0.204 228.3
C (mp-66) <1 1 0> <1 0 -1> 0.205 275.3
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.208 252.1
MgF2 (mp-1249) <1 1 0> <0 1 0> 0.208 227.4
ZnSe (mp-1190) <1 0 0> <1 0 1> 0.220 167.3
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.226 252.1
GaSe (mp-1943) <0 0 1> <1 0 0> 0.237 217.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
266 101 112 0 -18 0
101 195 99 0 38 0
112 99 187 0 -5 0
0 0 0 65 0 26
-18 38 -5 0 88 0
0 0 0 26 0 61
Compliance Tensor Sij (10-12Pa-1)
5.6 -2.2 -2.1 0 2.0 0
-2.2 9.0 -3.6 0 -4.6 0
-2.1 -3.6 8.6 0 1.6 0
0 0 0 18.6 0 -7.9
2.0 -4.6 1.6 0 13.8 0
0 0 0 -7.9 0 19.7
Shear Modulus GV
65 GPa
Bulk Modulus KV
141 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
136 GPa
Shear Modulus GVRH
59 GPa
Bulk Modulus KVRH
139 GPa
Elastic Anisotropy
1.15
Poisson's Ratio
0.31

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.35 0.00 0.00
0.00 3.28 0.00
0.00 0.00 3.09
Dielectric Tensor εij (total)
9.86 0.00 -0.62
0.00 9.11 0.00
-0.62 0.00 8.78
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.24
Polycrystalline dielectric constant εpoly
(total)
9.25
Refractive Index n
1.80
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Lu2Si2O7 (mp-7193) 0.1210 0.000 3
Er2Si2O7 (mp-7064) 0.0560 0.000 3
In2Si2O7 (mp-2874) 0.1500 0.005 3
Yb2Si2O7 (mp-4300) 0.1727 0.022 3
Tm2Si2O7 (mp-1095467) 0.0872 0.000 3
LiBiP2O7 (mp-759568) 0.5209 0.060 4
LiVP2O7 (mp-766613) 0.3854 0.031 4
LiCrP2O7 (mp-777633) 0.3595 2.061 4
SrV2P2O9 (mp-25797) 0.6629 0.040 4
LiFeP2O7 (mp-687079) 0.4395 0.208 4
LiMn3P3(HO6)2 (mp-780879) 0.7295 0.319 5
CaVNiP2O9 (mp-25785) 0.6962 0.161 5
Co3AgP3(HO6)2 (mp-25684) 0.7270 0.246 5
CaFeNiP2O9 (mvc-8266) 0.7279 0.278 5
CaCrNiP2O9 (mvc-8343) 0.7167 0.277 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Si O
Final Energy/Atom
-8.5394 eV
Corrected Energy
-98.8500 eV
-98.8500 eV = -93.9339 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 281313
  • 281312
Submitted by
User remarks:
  • Diyttrium disilicate - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)