material

Zn(GaO2)2

ID:

mp-5794

DOI:

10.17188/1276697


Tags: Zinc digallium oxide Zinc digallium tetraoxide Spinel-(Zn,Ga) Zinc digallate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.186 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.90 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.312 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 9394 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.000 286.2
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.010 101.2
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.011 214.7
Cu (mp-30) <1 1 0> <1 1 0> 0.019 202.4
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.021 123.9
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.021 123.9
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.033 143.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.033 71.6
PbS (mp-21276) <1 1 0> <1 1 0> 0.036 101.2
InP (mp-20351) <1 0 0> <1 0 0> 0.042 71.6
InP (mp-20351) <1 1 0> <1 1 0> 0.046 101.2
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.057 123.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.094 71.6
MgO (mp-1265) <1 0 0> <1 0 0> 0.102 71.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.110 101.2
MgO (mp-1265) <1 1 1> <1 1 1> 0.113 123.9
ZnO (mp-2133) <1 1 1> <1 0 0> 0.114 286.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.143 214.7
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.183 286.2
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.194 71.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.209 286.2
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.209 101.2
Fe3O4 (mp-19306) <1 1 1> <1 1 1> 0.214 123.9
NaCl (mp-22862) <1 0 0> <1 0 0> 0.217 286.2
Ni (mp-23) <1 1 1> <1 0 0> 0.264 214.7
GaN (mp-804) <1 0 1> <1 0 0> 0.314 214.7
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.334 286.2
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.384 286.2
Mg (mp-153) <1 0 0> <1 0 0> 0.387 286.2
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.397 286.2
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.438 214.7
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.445 143.1
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.458 286.2
LiF (mp-1138) <1 0 0> <1 1 1> 0.508 247.9
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.548 286.2
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.591 202.4
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.804 286.2
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.847 286.2
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.856 286.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.982 286.2
SiO2 (mp-6930) <1 1 1> <1 1 0> 1.086 101.2
TeO2 (mp-2125) <1 0 0> <1 1 0> 1.512 202.4
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 1.777 286.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
233 136 136 0 0 0
136 233 136 0 0 0
136 136 233 0 0 0
0 0 0 106 0 0
0 0 0 0 106 0
0 0 0 0 0 106
Compliance Tensor Sij (10-12Pa-1)
7.5 -2.8 -2.8 0 0 0
-2.8 7.5 -2.8 0 0 0
-2.8 -2.8 7.5 0 0 0
0 0 0 9.4 0 0
0 0 0 0 9.4 0
0 0 0 0 0 9.4
Shear Modulus GV
83 GPa
Bulk Modulus KV
169 GPa
Shear Modulus GR
72 GPa
Bulk Modulus KR
169 GPa
Shear Modulus GVRH
78 GPa
Bulk Modulus KVRH
169 GPa
Elastic Anisotropy
0.77
Poisson's Ratio
0.30

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.22 0.00 0.00
0.00 4.22 -0.00
0.00 -0.00 4.22
Dielectric Tensor εij (total)
11.78 0.00 0.00
0.00 11.78 -0.00
0.00 -0.00 11.78
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.22
Polycrystalline dielectric constant εpoly
(total)
11.78
Refractive Index n
2.05
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCr2O4 (mp-19410) 0.0090 0.000 3
Ga2CoO4 (mp-765889) 0.0050 0.000 3
Gd2CdO4 (mp-754093) 0.0027 1.567 3
Ti2MnO4 (mp-566588) 0.0195 0.073 3
ZnCr2O4 (mvc-11550) 0.0089 0.000 3
Li2MnCo3O8 (mp-761737) 0.0537 0.028 4
Li2NbCr3O8 (mp-774088) 0.0653 0.015 4
Li2Fe3CuO8 (mp-772689) 0.0602 0.046 4
Li2V3CoO8 (mp-765546) 0.0613 0.223 4
Li2Ti3CrO8 (mp-771759) 0.0385 0.005 4
Co3O4 (mp-559191) 0.1582 0.046 2
In3S4 (mp-556597) 0.0993 0.042 2
Co3O4 (mp-18748) 0.1057 0.046 2
Sn3N4 (mp-16031) 0.1214 0.000 2
Ge3N4 (mp-476) 0.1582 0.109 2
Li4Cr2Fe3Co3O16 (mp-775698) 0.3956 0.109 5
Li14Mn22Cr3Cu3O56 (mp-735790) 0.3646 0.014 5
Li4Mn3Cr3(CuO8)2 (mp-765456) 0.3688 0.069 5
Li4Cr3Cu3(SbO8)2 (mp-783908) 0.3957 0.035 5
Li4Cr3Fe3(SbO8)2 (mp-771925) 0.4035 0.047 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Illustration of the formation of a mesoporous colloidal template and an ion-exchange reaction based on the colloidal template. a)NaGaO2 solid powder particles. b)NaGaO2 colloidal particles obtained [...]
Au-functionalized ZnGa2O4 nanowires were synthesized on Si substrates by thermal evaporation followed by the sputter-deposition of Au and thermal annealing. 1D ZnGa2O3 structures were first synthesize [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Zn(GaO2)2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Ga_d O
Final Energy/Atom
-5.6569 eV
Corrected Energy
-84.8152 eV
-84.8152 eV = -79.1968 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 81106
  • 81108
  • 81112
  • 290017
  • 81105
  • 81113
  • 81107
  • 290667
  • 9394
  • 81111
  • 81109
  • 81110
  • 187290
Submitted by
User remarks:
  • Zinc digallium oxide
  • Spinel-(Zn,Ga)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)