Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.661 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.42 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.056 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 53070 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 0> <1 1 0> 0.003 49.1
Au (mp-81) <1 0 0> <1 0 0> 0.003 34.7
Al (mp-134) <1 0 0> <1 0 0> 0.004 277.9
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.008 60.2
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.009 173.7
Ag (mp-124) <1 1 0> <1 1 0> 0.009 49.1
Ag (mp-124) <1 0 0> <1 0 0> 0.010 34.7
GaSe (mp-1943) <0 0 1> <1 1 1> 0.011 240.6
Cu (mp-30) <1 1 0> <1 1 0> 0.015 147.4
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.015 277.9
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.018 147.4
GaTe (mp-542812) <1 0 0> <1 1 1> 0.023 180.5
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.023 312.6
GaN (mp-804) <0 0 1> <1 1 1> 0.023 240.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.033 277.9
SiC (mp-8062) <1 0 0> <1 0 0> 0.033 173.7
TePb (mp-19717) <1 0 0> <1 0 0> 0.044 173.7
LaF3 (mp-905) <0 0 1> <1 1 1> 0.054 180.5
PbSe (mp-2201) <1 0 0> <1 0 0> 0.055 312.6
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.062 277.9
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.062 343.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.067 173.7
GaN (mp-804) <1 0 1> <1 0 0> 0.070 208.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.071 138.9
GaSb (mp-1156) <1 0 0> <1 0 0> 0.095 312.6
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.096 312.6
WS2 (mp-224) <0 0 1> <1 1 1> 0.102 240.6
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.103 240.6
GaTe (mp-542812) <0 0 1> <1 1 1> 0.111 300.8
Au (mp-81) <1 1 1> <1 0 0> 0.112 243.1
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.117 60.2
Mg (mp-153) <1 0 1> <1 0 0> 0.126 208.4
CsI (mp-614603) <1 0 0> <1 0 0> 0.133 312.6
CdTe (mp-406) <1 0 0> <1 0 0> 0.134 173.7
CdSe (mp-2691) <1 0 0> <1 0 0> 0.136 312.6
SiC (mp-8062) <1 1 0> <1 1 0> 0.136 294.7
Te2W (mp-22693) <0 1 1> <1 1 0> 0.152 294.7
InSb (mp-20012) <1 0 0> <1 0 0> 0.164 173.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.165 180.5
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.167 312.6
Mg (mp-153) <0 0 1> <1 1 0> 0.183 245.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.191 343.8
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.192 277.9
GaN (mp-804) <1 1 1> <1 0 0> 0.201 277.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.204 173.7
Ag (mp-124) <1 1 1> <1 0 0> 0.213 243.1
WS2 (mp-224) <1 1 1> <1 1 1> 0.215 240.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.221 138.9
CdS (mp-672) <1 0 0> <1 0 0> 0.235 173.7
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.236 180.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
258 83 83 0 0 0
83 258 83 0 0 0
83 83 258 0 0 0
0 0 0 68 0 0
0 0 0 0 68 0
0 0 0 0 0 68
Compliance Tensor Sij (10-12Pa-1)
4.6 -1.1 -1.1 0 0 0
-1.1 4.6 -1.1 0 0 0
-1.1 -1.1 4.6 0 0 0
0 0 0 14.7 0 0
0 0 0 0 14.7 0
0 0 0 0 0 14.7
Shear Modulus GV
76 GPa
Bulk Modulus KV
142 GPa
Shear Modulus GR
75 GPa
Bulk Modulus KR
142 GPa
Shear Modulus GVRH
75 GPa
Bulk Modulus KVRH
142 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.27

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -1.12793 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -1.12793 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -1.12793
Piezoelectric Modulus ‖eijmax
1.12793 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
20.46 0.00 0.00
0.00 20.46 0.00
0.00 0.00 20.46
Dielectric Tensor εij (total)
31.64 0.00 0.00
0.00 31.64 0.00
0.00 0.00 31.64
Polycrystalline dielectric constant εpoly
(electronic contribution)
20.46
Polycrystalline dielectric constant εpoly
(total)
31.64
Refractive Index n
4.52
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZrCoSb (mp-22377) 0.0000 0.609 3
LiZnP (mp-10182) 0.0000 0.000 3
LiNdSn (mp-12719) 0.0000 0.169 3
YbSbPd (mp-10981) 0.0000 0.771 3
TiNiSb (mp-20952) 0.0000 0.000 3
SrCl2 (mp-23209) 0.0000 0.000 2
Mg2Pb (mp-20724) 0.0000 0.000 2
Li2Se (mp-2286) 0.0000 0.000 2
SmH2 (mp-24658) 0.0000 0.000 2
CrH2 (mp-24208) 0.0000 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Co Sb
Final Energy/Atom
-7.0388 eV
Corrected Energy
-21.1163 eV
-21.1163 eV = -21.1163 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 169147
  • 169164
  • 169151
  • 169163
  • 169152
  • 169149
  • 169162
  • 169142
  • 624920
  • 169148
  • 169157
  • 169153
  • 624919
  • 169165
  • 169143
  • 169140
  • 169144
  • 169155
  • 169156
  • 169150
  • 169139
  • 169138
  • 169154
  • 169141
  • 53070
  • 169159
  • 169146
  • 169158
  • 169160
  • 169161
  • 169145
Submitted by
User remarks:
  • Titanium cobalt antimony (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)