Final Magnetic Moment0.013 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.905 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPNCl2 + PCl3O + PNO + S8O + N2 |
Band Gap2.612 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 142.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 161.1 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 177.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 222.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 222.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 142.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 222.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 161.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 222.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 296.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 142.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 222.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 296.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 222.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 142.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 296.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 296.4 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 142.0 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 296.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 160.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 296.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 177.4 |
C (mp-48) | <1 0 1> | <0 0 1> | 296.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 222.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 222.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 222.3 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 177.4 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 296.4 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 142.0 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 296.4 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 222.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 296.4 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 222.3 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 296.4 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 296.4 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 222.3 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 296.4 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 148.2 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 148.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 222.3 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 177.4 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 0> | 142.0 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 296.4 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 142.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PNCl2 (mp-23375) | 0.3841 | 0.004 | 3 |
PBr2N (mp-23457) | 0.3528 | 0.004 | 3 |
P2S2O3 (mp-3667) | 0.4836 | 0.000 | 3 |
S3N2O5 (mp-29224) | 0.4315 | 0.187 | 3 |
PNF2 (mp-560275) | 0.5026 | 0.015 | 3 |
PBrNF (mp-559366) | 0.5272 | 0.014 | 4 |
PNClF (mp-554472) | 0.4081 | 0.008 | 4 |
SNClO (mp-558844) | 0.4097 | 0.274 | 4 |
P6N6Cl10O (mp-680008) | 0.2540 | 0.012 | 4 |
SNClO (mp-667281) | 0.3583 | 0.292 | 4 |
CrO3 (mp-776563) | 0.5044 | 0.101 | 2 |
P2O5 (mp-562613) | 0.5199 | 0.010 | 2 |
SeO3 (mp-27519) | 0.5709 | 0.018 | 2 |
SO3 (mp-2414) | 0.5027 | 0.000 | 2 |
P2O5 (mp-2452) | 0.5271 | 0.000 | 2 |
PS2N3(Cl2O)2 (mp-559089) | 0.3695 | 0.240 | 5 |
FeTeS2N2Cl5 (mp-638705) | 0.6639 | 0.216 | 5 |
P2SN3Cl5O (mp-556186) | 0.3703 | 0.139 | 5 |
H8CN2(ClO5)2 (mp-560730) | 0.6496 | 0.540 | 5 |
CS4N2(OF)3 (mp-555309) | 0.5861 | 0.203 | 5 |
NaH2CSO4F3 (mp-601228) | 0.7157 | 0.722 | 6 |
LiC2S2N(O2F3)2 (mp-557395) | 0.6407 | 0.216 | 6 |
CSe2S2N2(OF)3 (mp-555329) | 0.5684 | 0.222 | 6 |
PS2N3Cl2(OF)2 (mp-558888) | 0.5362 | 0.278 | 6 |
VP2C4N3(ClF6)2 (mp-693133) | 0.5564 | 0.479 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P S N Cl O |
Final Energy/Atom-5.3360 eV |
Corrected Energy-304.2804 eV
-304.2804 eV = -298.8174 eV (uncorrected energy) - 5.4630 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)