material

C

ID:

mp-66

DOI:

10.17188/1281384

Warnings: [?]
  1. Large change in a lattice parameter during relaxation.
  2. Large change in volume during relaxation.

Tags: Diamond 3C Carbon Carbon - diamond Carbon - cubic diamond Diamond High pressure experimental phase

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.135 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.135 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
C
Band Gap
4.114 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 28857 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 0 0> <1 0 0> 0.000 319.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.001 54.2
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.001 22.1
SiC (mp-7631) <1 1 0> <1 1 0> 0.003 162.6
GaSe (mp-1943) <0 0 1> <1 1 1> 0.004 88.5
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.005 54.2
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.005 66.4
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.008 154.9
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.008 63.9
Si (mp-149) <1 1 1> <1 1 1> 0.011 154.9
InAs (mp-20305) <1 1 0> <1 1 0> 0.011 54.2
InAs (mp-20305) <1 1 1> <1 1 1> 0.011 66.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.035 63.9
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.048 76.7
CdSe (mp-2691) <1 1 0> <1 1 0> 0.053 54.2
CdSe (mp-2691) <1 1 1> <1 1 1> 0.054 66.4
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.060 191.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.063 63.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.064 115.0
KP(HO2)2 (mp-23959) <0 1 1> <1 1 0> 0.066 108.4
WS2 (mp-224) <1 0 1> <1 0 0> 0.069 230.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.077 217.2
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.078 115.0
CaCO3 (mp-3953) <1 0 1> <1 0 0> 0.081 89.4
GaSb (mp-1156) <1 1 0> <1 1 0> 0.088 54.2
GaSb (mp-1156) <1 1 1> <1 1 1> 0.089 66.4
BN (mp-984) <1 0 1> <1 1 0> 0.119 162.6
GaSe (mp-1943) <1 0 0> <1 0 0> 0.122 268.3
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.125 66.4
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.127 66.4
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.134 115.0
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.140 162.6
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.140 76.7
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.142 199.2
PbSe (mp-2201) <1 1 0> <1 1 0> 0.145 54.2
PbSe (mp-2201) <1 1 1> <1 1 1> 0.147 66.4
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.152 63.9
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.158 162.6
BN (mp-984) <0 0 1> <1 1 1> 0.159 22.1
ZnO (mp-2133) <0 0 1> <1 1 1> 0.166 66.4
SiC (mp-8062) <1 1 1> <1 0 0> 0.181 268.3
GaN (mp-804) <1 1 0> <1 1 0> 0.186 325.3
SiC (mp-8062) <1 0 0> <1 1 1> 0.198 154.9
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.206 153.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.210 63.9
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.217 22.1
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.221 144.6
BN (mp-984) <1 1 1> <1 1 0> 0.235 271.1
KCl (mp-23193) <1 0 0> <1 0 0> 0.240 166.1
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.245 162.6
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
4.69 J/m2 (0.29 eV/Å2)
Weighted work function Φ
4.76 eV
Shape factor η
5.02
Surface energy anisotropy αγ
0.008
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(331) 4.66, 0.29 4.64 0.73
(100) * 4.74, 0.30 5.17 0.24
(221) 4.79, 0.30 4.53 0.03
(111) 5.03, 0.31 4.02 0.00
(110) 5.21, 0.33 5.23 0.00
(322) 5.30, 0.33 4.35 0.00
(320) 5.57, 0.35 5.28 0.00
(321) 5.69, 0.35 4.89 0.00
(210) 5.69, 0.36 5.86 0.00
(211) 5.78, 0.36 5.17 0.00
(311) 6.07, 0.38 5.51 0.00
(332) 6.78, 0.42 5.69 0.00
(310) 6.88, 0.43 5.62 0.00
(100) 8.45, 0.53 7.00 0.00

* indicates reconstructed surface.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
1054 126 126 0 0 0
126 1054 126 0 0 0
126 126 1054 0 0 0
0 0 0 562 0 0
0 0 0 0 562 0
0 0 0 0 0 562
Compliance Tensor Sij (10-12Pa-1)
1.0 -0.1 -0.1 0.0 0.0 0.0
-0.1 1.0 -0.1 -0.0 0.0 -0.0
-0.1 -0.1 1.0 0.0 -0.0 0.0
0.0 -0.0 0.0 1.8 -0.0 0.0
0.0 0.0 -0.0 -0.0 1.8 -0.0
0.0 -0.0 0.0 0.0 -0.0 1.8
Shear Modulus GV
523 GPa
Bulk Modulus KV
436 GPa
Shear Modulus GR
518 GPa
Bulk Modulus KR
436 GPa
Shear Modulus GVRH
520 GPa
Bulk Modulus KVRH
436 GPa
Elastic Anisotropy
0.04
Poisson's Ratio
0.07

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.83 0.00 0.00
0.00 5.83 0.00
0.00 0.00 5.83
Dielectric Tensor εij (total)
5.83 0.00 0.00
0.00 5.83 0.00
0.00 0.00 5.83
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.83
Polycrystalline dielectric constant εpoly
(total)
5.83
Refractive Index n
2.41
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn3CrS4 (mp-1080726) 0.0175 0.123 3
Zn3CrSe4 (mp-1095028) 0.0124 0.118 3
Zn3CrTe4 (mp-1087545) 0.0105 0.113 3
CdSnSb2 (mp-10063) 0.0250 0.000 3
GaCuS2 (mp-5238) 0.0192 0.000 3
FeCu2GeS4 (mp-917359) 0.0383 0.041 4
CoCu2GeS4 (mp-6498) 0.0382 0.061 4
CoCu2GeS4 (mp-560428) 0.0476 0.061 4
FeCu2GeS4 (mp-22053) 0.0260 0.041 4
FeCu2GeSe4 (mp-1087471) 0.0871 0.038 4
TcC (mp-1009848) 0.0000 0.556 2
PdC (mp-1009538) 0.0000 1.214 2
MgAl (mp-1038818) 0.0000 0.925 2
CaSe (mp-1008223) 0.0000 0.258 2
AgN (mp-1009766) 0.0000 1.537 2
O2 (mp-1057818) 0.0000 1.947 1
Si (mp-149) 0.0000 0.000 1
Sn (mp-117) 0.0000 0.000 1
Ge (mp-32) 0.0000 0.000 1
Se (mp-12771) 0.0000 0.509 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: C
Final Energy/Atom
-9.0903 eV
Corrected Energy
-18.1806 eV
-18.1806 eV = -18.1806 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 44101
  • 248466
  • 182270
  • 28858
  • 28862
  • 67787
  • 28861
  • 28859
  • 44100
  • 52054
  • 53779
  • 28860
  • 655131
  • 66464
  • 28857
  • 29068
  • 248465
  • 190652
  • 76766
  • 168170
  • 190651
  • 656475
  • 182729
  • 190653
  • 191804
  • 190650
  • 28863
  • 187639
  • 29151
Submitted by
User remarks:
  • Carbon
  • Diamond

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)