material

Mg3Hg

ID:

mp-731

DOI:

10.17188/1287669


Tags: Magnesium mercury (3/1) Mercury magnesium (1/3)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.115 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.043 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg3Hg
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 104316 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 1 1> <0 0 1> 0.000 270.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.001 62.3
PbS (mp-21276) <1 1 0> <1 1 1> 0.006 152.3
Au (mp-81) <1 1 1> <0 0 1> 0.008 270.0
C (mp-48) <1 1 1> <0 0 1> 0.009 270.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.010 270.0
GaN (mp-804) <0 0 1> <0 0 1> 0.016 62.3
Cu (mp-30) <1 1 1> <0 0 1> 0.018 270.0
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.018 311.5
GaSb (mp-1156) <1 1 1> <0 0 1> 0.022 270.0
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.022 228.5
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.023 228.5
WS2 (mp-224) <0 0 1> <0 0 1> 0.034 62.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.034 62.3
CdSe (mp-2691) <1 1 1> <0 0 1> 0.034 270.0
BN (mp-984) <1 1 0> <0 0 1> 0.037 270.0
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.044 332.3
InP (mp-20351) <1 1 0> <1 1 1> 0.045 152.3
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.048 293.1
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.048 228.5
CdS (mp-672) <1 0 0> <0 0 1> 0.049 228.5
Te2W (mp-22693) <0 0 1> <0 0 1> 0.054 311.5
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.056 166.2
KCl (mp-23193) <1 1 0> <1 1 1> 0.057 228.5
Ag (mp-124) <1 0 0> <0 0 1> 0.059 103.8
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.063 332.3
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.064 270.0
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.065 211.5
ZnO (mp-2133) <1 1 0> <1 0 1> 0.065 329.9
InP (mp-20351) <1 1 1> <0 0 1> 0.071 62.3
Mg (mp-153) <0 0 1> <0 0 1> 0.072 62.3
Au (mp-81) <1 0 0> <0 0 1> 0.072 103.8
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.072 235.6
MgO (mp-1265) <1 1 0> <0 0 1> 0.078 103.8
C (mp-48) <1 1 0> <0 0 1> 0.078 270.0
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.083 166.2
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.084 332.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.085 83.1
BN (mp-984) <0 0 1> <0 0 1> 0.088 145.4
C (mp-48) <0 0 1> <0 0 1> 0.090 20.8
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.090 145.4
C (mp-48) <1 0 1> <1 0 1> 0.094 235.6
NaCl (mp-22862) <1 0 0> <1 1 0> 0.094 293.1
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.095 145.4
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.097 270.0
SiC (mp-8062) <1 0 0> <0 0 1> 0.097 290.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.098 270.0
ZnSe (mp-1190) <1 0 0> <1 1 0> 0.098 293.1
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.098 296.1
CdS (mp-672) <0 0 1> <0 0 1> 0.100 62.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
62 47 18 0 0 0
47 62 18 0 0 0
18 18 100 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 7
Compliance Tensor Sij (10-12Pa-1)
38.3 -28.6 -1.7 0 0 0
-28.6 38.3 -1.7 0 0 0
-1.7 -1.7 10.7 0 0 0
0 0 0 54.5 0 0
0 0 0 0 54.5 0
0 0 0 0 0 133.8
Shear Modulus GV
18 GPa
Bulk Modulus KV
43 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
43 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
43 GPa
Elastic Anisotropy
2.33
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CuP (mp-675589) 0.3875 0.020 3
Li2CuP (mp-12029) 0.4542 0.000 3
ZrAlPt2 (mp-10906) 0.2003 0.677 3
Li2CuAs (mp-15686) 0.4122 0.000 3
HfAlPt2 (mp-1078728) 0.2038 0.695 3
LaF3 (mp-8354) 0.0128 0.020 2
K3P (mp-7897) 0.0358 0.010 2
CeF3 (mp-557720) 0.0327 0.027 2
K3As (mp-14018) 0.0157 0.000 2
Rb3As (mp-7898) 0.0208 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Hg
Final Energy/Atom
-1.3889 eV
Corrected Energy
-11.1114 eV
-11.1114 eV = -11.1114 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104316
  • 639092
  • 639082
Submitted by
User remarks:
  • Mercury magnesium (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)