material

NaCuTe

ID:

mp-7434

DOI:

10.17188/1287980


Tags: Copper sodium telluride (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.477 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.17 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Na2Te + CuTe + Cu
Band Gap
0.633 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 12156 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 0 0> <0 0 1> 0.001 38.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.002 173.5
SiC (mp-8062) <1 1 1> <1 1 0> 0.003 132.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.003 250.6
SiC (mp-7631) <0 0 1> <1 1 0> 0.003 132.8
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.003 219.2
GaSb (mp-1156) <1 0 0> <0 0 1> 0.003 38.6
SiC (mp-11714) <0 0 1> <1 1 0> 0.004 132.8
LaAlO3 (mp-2920) <0 0 1> <1 1 0> 0.004 177.1
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.007 281.8
SiC (mp-8062) <1 0 0> <0 0 1> 0.008 19.3
ZnO (mp-2133) <0 0 1> <1 1 0> 0.009 177.1
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.009 154.2
PbSe (mp-2201) <1 0 0> <0 0 1> 0.011 38.6
CdS (mp-672) <0 0 1> <1 0 1> 0.011 183.8
TePb (mp-19717) <1 0 0> <0 0 1> 0.012 173.5
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.012 327.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.015 57.8
AlN (mp-661) <0 0 1> <0 0 1> 0.015 134.9
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.018 144.9
Te2W (mp-22693) <0 1 1> <1 0 1> 0.020 294.2
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.020 38.6
Ga2O3 (mp-886) <1 0 -1> <1 1 1> 0.022 193.2
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.024 281.8
InAs (mp-20305) <1 0 0> <0 0 1> 0.026 38.6
Te2Mo (mp-602) <0 0 1> <1 1 0> 0.027 44.3
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.027 154.2
MgO (mp-1265) <1 1 1> <0 0 1> 0.027 347.0
C (mp-66) <1 1 1> <0 0 1> 0.030 154.2
Al2O3 (mp-1143) <1 1 0> <1 0 1> 0.031 110.3
ZnO (mp-2133) <1 1 1> <1 1 0> 0.031 221.4
Bi2Se3 (mp-541837) <0 0 1> <1 0 1> 0.032 183.8
Ag (mp-124) <1 1 0> <1 0 0> 0.033 219.2
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.035 250.6
Ag (mp-124) <1 0 0> <0 0 1> 0.035 154.2
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.036 257.4
CaCO3 (mp-3953) <1 1 1> <0 0 1> 0.037 154.2
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.039 281.8
CdTe (mp-406) <1 1 0> <1 1 0> 0.039 310.0
PbSe (mp-2201) <1 1 0> <1 1 0> 0.041 221.4
BN (mp-984) <1 1 0> <0 0 1> 0.041 134.9
InSb (mp-20012) <1 1 0> <1 1 0> 0.042 310.0
BN (mp-984) <0 0 1> <1 0 1> 0.042 110.3
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.047 221.4
Te2Mo (mp-602) <1 1 1> <0 0 1> 0.048 96.4
Au (mp-81) <1 1 0> <1 0 0> 0.050 219.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.051 154.2
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.052 281.8
GaSb (mp-1156) <1 1 0> <1 1 0> 0.053 221.4
NdGaO3 (mp-3196) <1 1 0> <1 1 1> 0.056 241.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
76 17 23 0 0 0
17 76 23 0 0 0
23 23 47 0 0 0
0 0 0 13 0 0
0 0 0 0 13 0
0 0 0 0 0 8
Compliance Tensor Sij (10-12Pa-1)
15.6 -1.2 -7.2 0 0 0
-1.2 15.6 -7.2 0 0 0
-7.2 -7.2 28.4 0 0 0
0 0 0 79.7 0 0
0 0 0 0 79.7 0
0 0 0 0 0 125.5
Shear Modulus GV
16 GPa
Bulk Modulus KV
36 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
35 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
36 GPa
Elastic Anisotropy
1.07
Poisson's Ratio
0.32

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
10.31 0.00 0.00
0.00 10.31 0.00
0.00 0.00 7.71
Dielectric Tensor εij (total)
16.41 0.00 0.00
0.00 16.41 0.00
0.00 0.00 13.65
Polycrystalline dielectric constant εpoly
(electronic contribution)
9.44
Polycrystalline dielectric constant εpoly
(total)
15.49
Refractive Index n
3.07
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiFeAs (mp-21471) 0.1422 0.000 3
CaMnSn (mp-20233) 0.0866 0.504 3
LiCoAs (mp-20698) 0.1473 0.000 3
LiFeAs (mp-917215) 0.1045 0.000 3
CaMnSn (mp-611471) 0.0883 0.504 3
Na2LiGaAs2 (mp-9722) 0.5239 0.000 4
Na2LiAlP2 (mp-9719) 0.6003 0.000 4
K2LiInAs2 (mp-505431) 0.5738 0.000 4
K3Na2SnBi3 (mp-568329) 0.5910 0.000 4
K2NaInSb2 (mp-505767) 0.5798 0.000 4
Fe2As (mp-20426) 0.6128 0.230 2
Mn2As (mp-1076981) 0.6363 0.065 2
SrAl2 (mp-1071777) 0.3361 0.013 2
Mg2Si (mp-1074652) 0.5434 0.088 2
TiH2 (mp-1077482) 0.6491 0.087 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Cu_pv Te
Final Energy/Atom
-3.3290 eV
Corrected Energy
-19.9738 eV
-19.9738 eV = -19.9738 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 12156
Submitted by
User remarks:
  • Copper sodium telluride (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)