Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.889 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + LiTi2(PO4)3 + Li3PO4 |
Band Gap2.406 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 196.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 327.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 327.1 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 151.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 196.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 261.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 327.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 250.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 196.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 196.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 261.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 196.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 250.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 130.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 196.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 151.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 327.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 196.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 196.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 327.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 327.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 327.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 261.7 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 196.2 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 262.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 261.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 261.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 196.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 261.7 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 261.7 |
Si (mp-149) | <1 1 0> | <0 0 1> | 327.1 |
Si (mp-149) | <1 1 1> | <0 0 1> | 196.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 151.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 196.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2V5O12 (mp-776871) | 0.5412 | 0.016 | 3 |
MgV3O8 (mp-767796) | 0.5576 | 0.010 | 3 |
Li2Cr4O13 (mp-770390) | 0.5404 | 0.020 | 3 |
Cr2P4O13 (mp-562181) | 0.5577 | 0.011 | 3 |
MgV3O8 (mp-705857) | 0.5428 | 0.009 | 3 |
NaFe2(MoO4)3 (mp-567233) | 0.3425 | 0.195 | 4 |
LiV2(PO4)3 (mp-540147) | 0.3286 | 0.084 | 4 |
LiCr2(PO4)3 (mp-31688) | 0.3433 | 0.079 | 4 |
LiFe2(PO4)3 (mp-997548) | 0.3256 | 0.065 | 4 |
LiTi2(PO4)3 (mp-774539) | 0.3239 | 0.007 | 4 |
V4O9 (mp-715664) | 0.7467 | 0.116 | 2 |
Li3Ti3Fe(PO4)6 (mp-743603) | 0.3600 | 0.026 | 5 |
Li9Nb10Cr6(PO4)24 (mp-851292) | 0.3239 | 0.031 | 5 |
Li2MnV(PO4)3 (mp-771376) | 0.3806 | 0.030 | 5 |
Li2MnV(PO4)3 (mp-770134) | 0.4157 | 0.028 | 5 |
Li2Zr7Fe(PO4)12 (mp-774285) | 0.3982 | 0.063 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.5569 | 0.173 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-744690) | 0.5180 | 0.193 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.4923 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5769 | 0.020 | 6 |
NaLi3Ti2Al2(PO4)6 (mp-776523) | 0.5724 | 0.036 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7222 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Fe_pv P O |
Final Energy/Atom-7.4712 eV |
Corrected Energy-592.0482 eV
-592.0482 eV = -552.8723 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|