Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.754 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2Sn2O3 |
Band Gap1.231 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 98.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 228.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 228.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 94.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 283.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 163.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 228.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 228.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 163.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 228.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 266.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 228.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 130.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 293.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 293.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 261.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 293.9 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 189.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 228.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 293.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 359.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 228.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 32.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 163.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 94.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 261.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 261.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 293.9 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 228.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 189.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 266.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 261.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 293.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 163.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 32.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 293.9 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 228.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 293.9 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 1> | 94.5 |
Si (mp-149) | <1 0 0> | <0 0 1> | 228.6 |
Si (mp-149) | <1 1 0> | <0 0 1> | 163.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 261.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 189.0 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 266.0 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 228.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 130.6 |
C (mp-48) | <1 0 0> | <1 0 0> | 266.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 293.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
124 | 44 | 53 | -10 | 0 | 0 |
44 | 124 | 53 | 10 | 0 | 0 |
53 | 53 | 130 | 0 | 0 | 0 |
-10 | 10 | 0 | 41 | 0 | 0 |
0 | 0 | 0 | 0 | 41 | -10 |
0 | 0 | 0 | 0 | -10 | 40 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.7 | -2.8 | -3.2 | 3.4 | 0 | 0 |
-2.8 | 10.7 | -3.2 | -3.4 | 0 | 0 |
-3.2 | -3.2 | 10.3 | 0 | 0 | 0 |
3.4 | -3.4 | 0 | 26.3 | 0 | 0 |
0 | 0 | 0 | 0 | 26.3 | 6.8 |
0 | 0 | 0 | 0 | 6.8 | 26.9 |
Shear Modulus GV39 GPa |
Bulk Modulus KV75 GPa |
Shear Modulus GR37 GPa |
Bulk Modulus KR75 GPa |
Shear Modulus GVRH38 GPa |
Bulk Modulus KVRH75 GPa |
Elastic Anisotropy0.29 |
Poisson's Ratio0.28 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.17 | -0.00 | -0.00 |
-0.00 | 5.17 | 0.00 |
-0.00 | 0.00 | 4.30 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.81 | -0.00 | -0.00 |
-0.00 | 11.81 | 0.00 |
-0.00 | 0.00 | 8.26 |
Polycrystalline dielectric constant
εpoly∞
4.88
|
Polycrystalline dielectric constant
εpoly
10.63
|
Refractive Index n2.21 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2Sn2O3 (mp-7863) | 0.3144 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sn_d O |
Final Energy/Atom-5.0286 eV |
Corrected Energy-37.3069 eV
-37.3069 eV = -35.2000 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)