Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.840 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.112 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2O + Li2CuP2O7 + Cu |
Band Gap0.323 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42m [121] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 135.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 212.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 160.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 222.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 154.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 290.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 174.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 38.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 56.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 280.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 38.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 56.6 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 280.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 359.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 290.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 160.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 222.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 251.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 222.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 251.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 251.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 309.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 38.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 160.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 174.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 154.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 222.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 320.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 240.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 154.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 154.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 311.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 320.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 77.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 355.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 320.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 154.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 226.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 251.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 359.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 266.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 251.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 120.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 96.7 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 282.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 96.7 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 282.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 226.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 290.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3VO4 (mp-780545) | 0.3485 | 0.000 | 3 |
Na3AsO4 (mp-756044) | 0.2804 | 0.000 | 3 |
Na3VO4 (mp-764673) | 0.1936 | 0.019 | 3 |
Li3PO4 (mp-13725) | 0.3028 | 0.000 | 3 |
VAg3O4 (mp-19412) | 0.1563 | 0.031 | 3 |
Li5Cu(PO4)2 (mp-779046) | 0.2700 | 0.031 | 4 |
Li2FeBO4 (mp-770663) | 0.2819 | 0.056 | 4 |
LiCu2PO4 (mp-760676) | 0.2789 | 0.108 | 4 |
LiCu2PO4 (mp-759287) | 0.2111 | 0.102 | 4 |
Li2CoBO4 (mp-771049) | 0.2793 | 0.300 | 4 |
ZnP2 (mp-2782) | 0.6964 | 0.000 | 2 |
ZnP2 (mp-680550) | 0.6542 | 0.190 | 2 |
Si3H (mp-995193) | 0.6296 | 0.033 | 2 |
Si3H (mp-1040468) | 0.6253 | 0.046 | 2 |
ZnP2 (mp-1392) | 0.6708 | 0.004 | 2 |
Si (mp-16220) | 0.7129 | 0.339 | 1 |
Si (mp-971661) | 0.5903 | 0.082 | 1 |
C (mp-1078845) | 0.7441 | 0.266 | 1 |
C (mp-1080826) | 0.7373 | 0.299 | 1 |
Si (mp-1095269) | 0.7073 | 0.096 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-5.9033 eV |
Corrected Energy-50.0353 eV
-50.0353 eV = -47.2262 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)