material

FePO4

ID:

mp-760343


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-2.334 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.38 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.821 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4 [82]
Hall
I 4
Point Group
1
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <0 0 1> 0.000 130.2
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.000 130.2
Al (mp-134) <1 0 0> <0 0 1> 0.000 130.2
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.001 208.4
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.001 52.1
Cu (mp-30) <1 0 0> <0 0 1> 0.002 26.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.002 234.4
NaCl (mp-22862) <1 0 0> <0 0 1> 0.002 130.2
ZnO (mp-2133) <1 0 0> <1 1 0> 0.003 226.1
GaN (mp-804) <1 0 1> <0 0 1> 0.004 286.5
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.006 130.2
BN (mp-984) <1 1 1> <1 0 0> 0.010 239.8
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.013 311.2
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.014 130.2
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.015 169.6
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.015 182.3
LaF3 (mp-905) <1 0 1> <1 1 0> 0.016 282.6
Cu (mp-30) <1 1 0> <0 0 1> 0.016 130.2
Cu (mp-30) <1 1 1> <0 0 1> 0.017 182.3
CdS (mp-672) <1 1 0> <1 1 1> 0.017 248.9
AlN (mp-661) <1 0 1> <1 0 0> 0.018 159.9
Ag (mp-124) <1 1 1> <0 0 1> 0.019 208.4
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.019 130.2
GaAs (mp-2534) <1 0 0> <0 0 1> 0.021 130.2
InAs (mp-20305) <1 0 0> <0 0 1> 0.021 338.6
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.021 182.3
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.022 130.2
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.024 279.8
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.024 338.6
CdWO4 (mp-19387) <0 1 1> <1 0 1> 0.025 286.2
WS2 (mp-224) <0 0 1> <1 0 1> 0.026 238.5
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.026 238.5
CdS (mp-672) <1 0 0> <0 0 1> 0.026 286.5
SiC (mp-11714) <1 0 0> <1 0 1> 0.027 95.4
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.028 104.2
Au (mp-81) <1 1 1> <0 0 1> 0.028 208.4
SiC (mp-7631) <1 0 1> <1 0 0> 0.029 239.8
KCl (mp-23193) <1 0 0> <0 0 1> 0.029 208.4
Mg (mp-153) <0 0 1> <1 0 1> 0.030 238.5
Si (mp-149) <1 1 0> <1 1 0> 0.030 169.6
LiTaO3 (mp-3666) <1 0 1> <1 1 0> 0.030 226.1
C (mp-66) <1 0 0> <0 0 1> 0.030 26.0
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.030 169.6
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.032 143.1
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.033 319.7
Ge (mp-32) <1 0 0> <0 0 1> 0.034 130.2
Te2W (mp-22693) <0 0 1> <1 0 0> 0.035 199.8
C (mp-48) <1 1 0> <1 1 0> 0.036 169.6
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.036 130.2
Mg (mp-153) <1 0 1> <0 0 1> 0.036 286.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.05162 0.11158 0.00000
0.00000 0.00000 0.00000 -0.11158 0.05162 0.00000
0.25530 -0.25530 0.00000 0.00000 0.00000 0.17337
Piezoelectric Modulus ‖eijmax
0.40052 C/m2
Crystallographic Direction vmax
-0.00000
-0.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.87 0.00 0.00
0.00 2.87 0.00
0.00 0.00 3.00
Dielectric Tensor εij (total)
5.21 0.00 0.00
0.00 5.21 0.00
0.00 0.00 5.89
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.91
Polycrystalline dielectric constant εpoly
(total)
5.44
Refractive Index n
1.71
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
FePO4 (mp-767830) 0.1448 0.009 3
FePO4 (mp-540111) 0.1682 0.005 3
GaPO4 (mp-677335) 0.1767 0.000 3
FePO4 (mp-19109) 0.1926 0.007 3
FePO4 (mp-686962) 0.1491 0.005 3
CsBeAsO4 (mp-9113) 0.6771 0.000 4
KSi2BO6 (mp-1019889) 0.5992 0.000 4
K2Al2Si3O10 (mp-1019744) 0.7131 0.018 4
LiB(SO4)2 (mp-1020106) 0.6490 0.000 4
Cs2MgSi5O12 (mp-1019610) 0.7134 0.000 4
SiO2 (mp-555165) 0.5115 0.027 2
SiO2 (mp-600024) 0.5579 0.018 2
CeSe2 (mp-1080262) 0.4976 0.511 2
CeSe2 (mp-1080272) 0.4564 0.510 2
CeSe2 (mp-1080311) 0.3953 0.513 2
RbZnB(PO4)2 (mp-557658) 0.6840 0.000 5
CsZnB(PO4)2 (mp-560244) 0.6102 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Melt casting was performed within an airtight box furnace under an Ar protection following the procedure described in Ref. [11]. Briefly, stoichiometric amounts of FePO42H2O (Buddenheim KG, Germany) [...]
LiFePO4 powder was synthesized from an aqueous solution route [19]. LiH2PO4 and Fe(NO3)39H2O were first dissolved in two distinct containers. After slowly adding the lithium-based solution into the i [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition FePO4.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv P O
Final Energy/Atom
-7.1130 eV
Corrected Energy
-190.7283 eV
Uncorrected energy = -170.7123 eV Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV Corrected energy = -190.7283 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)