material

ZrCoO3

ID:

mp-761293

DOI:

10.17188/1291789


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-2.705 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.097 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.46 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ZrO2 + CoO
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
1
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 25.3
CdTe (mp-406) <1 1 1> <0 0 1> 0.001 76.0
InSb (mp-20012) <1 1 1> <0 0 1> 0.004 76.0
ZnO (mp-2133) <0 0 1> <0 0 1> 0.009 177.4
AlN (mp-661) <0 0 1> <0 0 1> 0.009 25.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.013 304.2
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.016 76.0
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.019 126.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.032 231.6
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.039 304.2
ZnO (mp-2133) <1 0 0> <0 0 1> 0.063 228.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.074 76.0
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.075 304.2
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.078 202.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.091 304.2
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.093 304.2
SiC (mp-11714) <1 1 0> <1 0 1> 0.102 162.5
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.112 152.1
C (mp-48) <0 0 1> <0 0 1> 0.114 101.4
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.117 133.7
Mg (mp-153) <0 0 1> <0 0 1> 0.161 329.5
TbScO3 (mp-31119) <0 1 1> <1 0 1> 0.167 162.5
SiC (mp-7631) <1 1 1> <1 0 1> 0.168 81.2
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.171 162.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.174 329.5
SiC (mp-11714) <1 1 1> <0 0 1> 0.189 278.8
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.197 253.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.200 304.2
ZnO (mp-2133) <1 1 0> <0 0 1> 0.213 152.1
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.214 329.5
SiC (mp-8062) <1 1 1> <0 0 1> 0.228 101.4
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.238 304.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.245 202.8
TePb (mp-19717) <1 1 1> <0 0 1> 0.254 76.0
SiC (mp-7631) <0 0 1> <0 0 1> 0.262 25.3
GaN (mp-804) <0 0 1> <0 0 1> 0.262 228.1
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.271 152.1
GaP (mp-2490) <1 0 0> <0 0 1> 0.273 152.1
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.274 253.5
BN (mp-984) <1 0 0> <0 0 1> 0.275 329.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.278 25.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.286 152.1
AlN (mp-661) <1 1 0> <0 0 1> 0.290 304.2
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.303 304.2
Mg (mp-153) <1 0 1> <0 0 1> 0.312 278.8
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.314 202.8
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.321 162.5
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.326 177.4
TiO2 (mp-390) <1 1 0> <1 0 0> 0.343 154.4
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.344 329.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
261 160 91 11 14 0
160 261 91 -11 -14 0
91 91 206 0 0 0
11 -11 0 44 0 -14
14 -14 0 0 44 11
0 0 0 -14 11 50
Compliance Tensor Sij (10-12Pa-1)
7.2 -4.3 -1.3 -2.8 -3.5 0
-4.3 7.2 -1.3 2.8 3.5 0
-1.3 -1.3 6 0 0 0
-2.8 2.8 0 26.2 0 7
-3.5 3.5 0 0 26.2 -5.7
0 0 0 7 -5.7 22.9
Shear Modulus GV
53 GPa
Bulk Modulus KV
157 GPa
Shear Modulus GR
45 GPa
Bulk Modulus KR
150 GPa
Shear Modulus GVRH
49 GPa
Bulk Modulus KVRH
153 GPa
Elastic Anisotropy
1.02
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnSnS3 (mp-1093994) 0.1371 0.169 3
LiMnF3 (mp-764337) 0.0862 0.040 3
LiMgH3 (mp-23736) 0.1393 0.009 3
NiSnO3 (mp-770398) 0.1531 0.026 3
CoSnO3 (mp-761574) 0.1150 0.035 3
Li3Nb4FeO12 (mp-771984) 0.3331 0.051 4
Mg2VWO6 (mvc-5881) 0.2870 0.022 4
Mg2TiWO6 (mvc-5939) 0.3131 0.125 4
InNi2SbO6 (mp-1078367) 0.2043 0.000 4
ScNi2SbO6 (mp-1078244) 0.3322 0.000 4
In2S3 (mp-22375) 0.1431 0.023 2
Sc2O3 (mp-755313) 0.1214 0.039 2
Ga2O3 (mp-1243) 0.1288 0.030 2
In2O3 (mp-22323) 0.1444 0.029 2
Fe2O3 (mp-796253) 0.1584 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.5302 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.6580 0.080 5
Li4MnV2WO12 (mp-773239) 0.7186 0.090 5
Li4Mn2TeWO12 (mp-768044) 0.6176 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6869 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Zr_sv Co O
Final Energy/Atom
-8.0650 eV
Corrected Energy
-176.0968 eV
Uncorrected energy = -161.3008 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV Corrected energy = -176.0968 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)