material

CoSnO3

ID:

mp-761574

DOI:

10.17188/1292099


Material Details

Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.749 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.035 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.34 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Co2SnO4 + SnO2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
1
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <0 0 1> 0.001 24.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.002 24.8
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.002 323.0
TePb (mp-19717) <1 1 1> <0 0 1> 0.002 74.5
SiC (mp-8062) <1 1 1> <0 0 1> 0.005 99.4
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.009 223.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.009 298.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.009 298.2
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.009 298.2
SiC (mp-11714) <1 1 1> <0 0 1> 0.017 273.3
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.039 347.9
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.043 173.9
C (mp-48) <0 0 1> <0 0 1> 0.045 99.4
Ge (mp-32) <1 1 1> <0 0 1> 0.048 173.9
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.074 198.8
WS2 (mp-224) <1 0 0> <1 0 0> 0.077 229.0
BN (mp-984) <1 0 1> <0 0 1> 0.085 223.6
TiO2 (mp-390) <0 0 1> <1 0 0> 0.088 229.0
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.093 323.0
TiO2 (mp-390) <1 1 1> <0 0 1> 0.095 273.3
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.097 372.7
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.113 323.0
GaAs (mp-2534) <1 1 1> <0 0 1> 0.114 173.9
Cu (mp-30) <1 1 1> <0 0 1> 0.117 298.2
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.119 173.9
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.124 323.0
SiC (mp-11714) <1 1 0> <1 0 1> 0.147 160.6
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.147 323.0
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.154 132.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.157 223.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.158 223.6
Al (mp-134) <1 1 0> <0 0 1> 0.170 372.7
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.170 173.9
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.171 223.6
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.190 124.2
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.197 74.5
C (mp-48) <1 0 1> <0 0 1> 0.234 372.7
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.237 372.7
Mg (mp-153) <0 0 1> <0 0 1> 0.265 223.6
SiC (mp-7631) <1 1 1> <1 0 1> 0.271 80.3
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.272 49.7
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.275 273.3
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.295 160.6
C (mp-48) <1 1 1> <1 0 1> 0.305 240.8
SiC (mp-7631) <1 1 0> <0 0 1> 0.307 248.5
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.318 24.8
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.319 248.5
CdTe (mp-406) <1 1 1> <0 0 1> 0.332 74.5
GaN (mp-804) <0 0 1> <0 0 1> 0.348 173.9
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.352 323.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
272 138 92 10 7 0
138 272 92 -10 -7 0
92 92 209 0 0 0
10 -10 0 45 0 -7
7 -7 0 0 45 10
0 0 0 -7 10 67
Compliance Tensor Sij (10-12Pa-1)
5.5 -2.4 -1.3 -1.7 -1.3 0
-2.4 5.5 -1.3 1.7 1.3 0
-1.3 -1.3 6 0 0 0
-1.7 1.7 0 23.2 0 2.6
-1.3 1.3 0 0 23.2 -3.4
0 0 0 2.6 -3.4 15.8
Shear Modulus GV
60 GPa
Bulk Modulus KV
155 GPa
Shear Modulus GR
55 GPa
Bulk Modulus KR
149 GPa
Shear Modulus GVRH
57 GPa
Bulk Modulus KVRH
152 GPa
Elastic Anisotropy
0.55
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMnF3 (mp-764337) 0.1031 0.040 3
LiMgH3 (mp-23736) 0.0805 0.009 3
ZrCoO3 (mp-761293) 0.1150 0.097 3
NiSnO3 (mp-770398) 0.1482 0.026 3
NaCdF3 (mp-4360) 0.1382 0.000 3
Mg2VWO6 (mvc-5881) 0.2642 0.022 4
Mg2TiWO6 (mvc-5939) 0.3031 0.125 4
Mg2CrWO6 (mvc-5960) 0.2930 0.670 4
InNi2SbO6 (mp-1078367) 0.1644 0.000 4
ScNi2SbO6 (mp-1078244) 0.3017 0.000 4
In2S3 (mp-22375) 0.1547 0.023 2
Sc2O3 (mp-755313) 0.1618 0.039 2
Ca3N2 (mp-1047) 0.1578 0.014 2
Fe2O3 (mp-714977) 0.1612 0.000 2
Fe2O3 (mp-796253) 0.1584 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.5073 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.6345 0.080 5
Li4MnV2WO12 (mp-773239) 0.7344 0.090 5
Li4Mn2TeWO12 (mp-768044) 0.5881 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6893 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Co Sn_d O
Final Energy/Atom
-6.2016 eV
Corrected Energy
-138.8277 eV
Uncorrected energy = -124.0317 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV Corrected energy = -138.8277 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)