material

As2Ru

ID:

mp-766

DOI:

10.17188/1296484


Tags: Ruthenium arsenide (1/2) Ruthenium(VI) arsenide Anduoite

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.398 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.05 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.495 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnnm [58]
Hall
-P 2 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 994 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 0 0> <1 1 0> 0.004 156.6
InSb (mp-20012) <1 0 0> <1 1 0> 0.005 352.4
AlN (mp-661) <1 0 0> <0 1 0> 0.006 94.2
CdTe (mp-406) <1 0 0> <1 1 0> 0.010 352.4
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.012 82.8
KCl (mp-23193) <1 1 1> <0 1 0> 0.013 282.7
GaP (mp-2490) <1 1 0> <1 0 0> 0.022 171.6
SiO2 (mp-6930) <1 0 1> <0 1 1> 0.029 175.6
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.031 190.6
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.033 132.5
Ag (mp-124) <1 0 0> <1 1 0> 0.035 156.6
GdScO3 (mp-5690) <0 0 1> <1 0 1> 0.041 190.6
TbScO3 (mp-31119) <0 0 1> <1 0 1> 0.048 190.6
Y3Fe5O12 (mp-19648) <1 0 0> <1 1 0> 0.065 156.6
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.070 149.0
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.071 132.5
Si (mp-149) <1 0 0> <0 0 1> 0.073 149.0
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.082 39.2
YAlO3 (mp-3792) <1 1 1> <0 0 1> 0.093 248.4
PbSe (mp-2201) <1 0 0> <1 1 0> 0.110 39.2
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.132 137.3
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.132 132.5
BN (mp-984) <0 0 1> <1 0 0> 0.142 137.3
Cu (mp-30) <1 1 1> <0 1 1> 0.152 225.8
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.152 265.0
LaF3 (mp-905) <0 0 1> <1 0 0> 0.158 137.3
CdS (mp-672) <0 0 1> <1 0 0> 0.170 137.3
GaSb (mp-1156) <1 0 0> <1 1 0> 0.170 39.2
DyScO3 (mp-31120) <0 0 1> <1 0 1> 0.178 190.6
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.179 132.5
Mg (mp-153) <1 1 0> <1 0 1> 0.185 114.3
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.187 281.5
InP (mp-20351) <1 0 0> <0 1 1> 0.187 250.9
PbS (mp-21276) <1 0 0> <0 1 1> 0.190 250.9
WSe2 (mp-1821) <1 1 0> <0 1 0> 0.202 263.8
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.221 82.8
CdSe (mp-2691) <1 0 0> <1 1 0> 0.229 39.2
KTaO3 (mp-3614) <1 1 1> <0 1 1> 0.249 250.9
AlN (mp-661) <0 0 1> <1 0 0> 0.263 34.3
ZnO (mp-2133) <1 0 1> <0 1 1> 0.265 100.3
C (mp-66) <1 1 0> <1 1 1> 0.274 127.5
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.277 150.8
GdScO3 (mp-5690) <0 1 1> <0 0 1> 0.278 165.6
InSb (mp-20012) <1 1 1> <1 0 0> 0.290 308.9
AlN (mp-661) <1 1 1> <1 0 1> 0.294 114.3
AlN (mp-661) <1 1 0> <0 0 1> 0.303 82.8
Fe2O3 (mp-24972) <1 1 0> <0 0 1> 0.313 248.4
Fe2O3 (mp-24972) <0 0 1> <0 1 1> 0.317 225.8
CdTe (mp-406) <1 1 1> <1 0 0> 0.325 308.9
LiTaO3 (mp-3666) <1 1 0> <0 0 1> 0.328 248.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
292 97 96 0 0 0
97 361 38 0 0 0
96 38 247 0 0 0
0 0 0 65 0 0
0 0 0 0 128 0
0 0 0 0 0 132
Compliance Tensor Sij (10-12Pa-1)
4.2 -1 -1.5 0 0 0
-1 3 -0.1 0 0 0
-1.5 -0.1 4.6 0 0 0
0 0 0 15.3 0 0
0 0 0 0 7.8 0
0 0 0 0 0 7.6
Shear Modulus GV
110 GPa
Bulk Modulus KV
151 GPa
Shear Modulus GR
100 GPa
Bulk Modulus KR
147 GPa
Shear Modulus GVRH
105 GPa
Bulk Modulus KVRH
149 GPa
Elastic Anisotropy
0.51
Poisson's Ratio
0.22

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
23.04 0.00 0.00
0.00 28.91 0.00
0.00 0.00 18.69
Dielectric Tensor εij (total)
34.98 0.00 0.00
0.00 39.47 0.00
0.00 0.00 38.84
Polycrystalline dielectric constant εpoly
(electronic contribution)
23.54
Polycrystalline dielectric constant εpoly
(total)
37.76
Refractive Index n
4.85
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
FeSbAs (mp-988996) 0.3588 0.024 3
Sb2Os (mp-2695) 0.1429 0.000 2
As2Os (mp-2455) 0.0945 0.000 2
FeAs2 (mp-2008) 0.0977 0.000 2
FeP2 (mp-20027) 0.0267 0.000 2
P2Ru (mp-1413) 0.1482 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: As Ru_pv
Final Energy/Atom
-6.5947 eV
Corrected Energy
-39.5680 eV
-39.5680 eV = -39.5680 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 42578
  • 611294
  • 611289
  • 994
Submitted by
User remarks:
  • Ruthenium arsenide (1/2)
  • Anduoite

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)