Li2CoO2

ID:

mp-755297


Material Details

Final Magnetic Moment
3.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.796 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.95 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Li10Co4O9 + CoO
Band Gap
2.552 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 1 1> <0 0 1> 0.002 266.9
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.004 177.7
GdScO3 (mp-5690) <0 0 1> <1 0 1> 0.006 128.2
GaSb (mp-1156) <1 1 1> <0 0 1> 0.007 266.9
ZnO (mp-2133) <0 0 1> <0 0 1> 0.009 111.9
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.009 60.3
BN (mp-984) <0 0 1> <0 0 1> 0.012 103.3
MgAl2O4 (mp-3536) <1 0 0> <1 0 1> 0.013 201.4
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.014 111.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.014 28.0
LiF (mp-1138) <1 0 0> <1 0 1> 0.017 201.4
PbSe (mp-2201) <1 1 1> <0 0 1> 0.018 266.9
GaTe (mp-542812) <0 0 1> <0 0 1> 0.019 301.3
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.019 84.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.021 266.9
Si (mp-149) <1 1 0> <1 1 0> 0.022 84.0
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.023 193.9
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.026 137.8
Te2W (mp-22693) <1 0 0> <1 0 0> 0.027 96.9
MgO (mp-1265) <1 1 0> <1 0 1> 0.028 128.2
InAs (mp-20305) <1 1 1> <0 0 1> 0.028 266.9
Cu (mp-30) <1 1 0> <1 1 0> 0.029 56.0
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.036 311.2
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.038 155.0
LaF3 (mp-905) <0 0 1> <0 0 1> 0.039 137.8
PbS (mp-21276) <1 1 0> <1 0 1> 0.040 256.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.041 60.3
Al (mp-134) <1 1 1> <0 0 1> 0.041 111.9
Ge (mp-32) <1 0 0> <1 0 1> 0.043 201.4
PbSe (mp-2201) <1 1 0> <0 0 1> 0.043 275.5
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.044 64.6
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.045 120.5
TiO2 (mp-390) <1 1 1> <0 0 1> 0.047 163.6
BN (mp-984) <1 1 1> <1 0 0> 0.047 274.7
BN (mp-984) <1 1 0> <0 0 1> 0.049 266.9
InSb (mp-20012) <1 1 0> <1 1 0> 0.051 251.9
GaTe (mp-542812) <1 1 0> <1 0 0> 0.053 193.9
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.053 146.4
GaSe (mp-1943) <1 1 1> <1 0 1> 0.056 238.0
KCl (mp-23193) <1 1 0> <0 0 1> 0.058 172.2
MoS2 (mp-1434) <1 1 0> <1 1 1> 0.063 117.1
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.063 163.6
WS2 (mp-224) <1 1 0> <1 1 1> 0.064 234.2
KP(HO2)2 (mp-23959) <1 1 0> <0 0 1> 0.068 137.8
KCl (mp-23193) <1 1 1> <0 0 1> 0.068 215.2
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.069 128.2
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.073 206.6
LaF3 (mp-905) <1 1 0> <0 0 1> 0.074 275.5
ZnO (mp-2133) <1 0 1> <0 0 1> 0.075 137.8
Si (mp-149) <1 0 0> <0 0 1> 0.078 206.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2NiO2 (mp-19308) 0.0681 0.046 3
Mg(AlSi)2 (mp-3833) 0.1789 0.056 3
Ca(CdP)2 (mp-9570) 0.1044 0.000 3
Ca(CdAs)2 (mp-7067) 0.1768 0.000 3
Eu(CdP)2 (mp-22609) 0.1524 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.1914 0.040 4
Li8VO5F (mp-765837) 0.7451 0.049 4
LiFeCuS2 (mp-755288) 0.3165 0.262 4
Mg3As2 (mp-7891) 0.1379 0.018 2
Be3N2 (mp-1017550) 0.3011 0.208 2
Pu2O3 (mp-21423) 0.2680 0.073 2
Mg3Sb2 (mp-2646) 0.2461 0.000 2
Sc2O3 (mp-13060) 0.1896 0.132 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Li_sv Co O
Final Energy/Atom
-5.3047 eV
Corrected Energy
-29.8019 eV
-29.8019 eV = -26.5233 eV (uncorrected energy) - 1.8740 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)