Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.310 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV4Fe2O13 + VO2 + Fe2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 -1> | 211.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 77.6 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 269.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 269.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 279.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 122.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 232.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 310.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 323.8 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 211.6 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 310.5 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 216.9 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 211.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 269.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 279.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 323.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 161.9 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 179.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 161.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 223.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 269.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 279.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 279.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 269.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 269.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 269.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 215.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 279.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 161.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 161.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 310.5 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 310.5 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 122.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 334.8 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 215.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 269.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 215.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 323.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 323.8 |
BN (mp-984) | <1 1 0> | <1 1 0> | 310.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 155.3 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 310.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 279.0 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 122.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 161.9 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 161.9 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 232.9 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 279.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 215.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 279.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2FeO6 (mp-773218) | 0.1868 | 0.020 | 3 |
V2CrO6 (mp-772127) | 0.1845 | 0.097 | 3 |
V5CoO12 (mp-761587) | 0.0522 | 0.174 | 3 |
V2NiO6 (mp-771872) | 0.1660 | 0.000 | 3 |
MnV5O12 (mp-776190) | 0.1246 | 0.061 | 3 |
MnV4NiO12 (mp-853162) | 0.1703 | 0.004 | 4 |
MnV4CrO12 (mp-771677) | 0.1482 | 0.057 | 4 |
V4FeCoO12 (mp-771474) | 0.1680 | 0.011 | 4 |
V4CrCoO12 (mp-771432) | 0.1540 | 0.059 | 4 |
V4CoNiO12 (mp-775042) | 0.1444 | 0.000 | 4 |
VO2 (mp-777469) | 0.7332 | 0.038 | 2 |
VO2 (mvc-6918) | 0.7114 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6050 | 0.281 | 2 |
Li2MnV(PO4)3 (mp-770179) | 0.4658 | 0.039 | 5 |
Li2MnV(PO4)3 (mp-770055) | 0.5064 | 0.030 | 5 |
Li2MnV(PO4)3 (mp-770169) | 0.4758 | 0.026 | 5 |
LiMnV(PO4)3 (mp-770143) | 0.4081 | 0.104 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.5087 | 0.130 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5413 | 0.257 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5203 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5136 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6514 | 0.331 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6302 | 0.001 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: V_pv Fe_pv O |
Final Energy/Atom-7.5156 eV |
Corrected Energy-154.8518 eV
-154.8518 eV = -135.2813 eV (uncorrected energy) - 11.1430 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)