material

C

ID:

mp-997182

DOI:

10.17188/1317207


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.004 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.004 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
1.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
C
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.000 68.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.000 68.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.000 84.4
C (mp-48) <0 0 1> <0 0 1> 0.001 5.3
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.005 184.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.010 111.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.017 111.0
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.027 68.6
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.039 259.1
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.051 111.0
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.054 226.8
Al (mp-134) <1 1 1> <0 0 1> 0.058 84.4
C (mp-48) <1 0 1> <0 0 1> 0.084 100.2
SiC (mp-8062) <1 1 1> <0 0 1> 0.099 100.2
CdTe (mp-406) <1 1 1> <0 0 1> 0.140 226.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.148 100.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.173 100.2
AlN (mp-661) <1 0 1> <0 0 1> 0.182 142.4
InSb (mp-20012) <1 1 1> <0 0 1> 0.198 226.8
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.238 111.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.246 126.6
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.253 259.1
Cu (mp-30) <1 1 1> <0 0 1> 0.256 68.6
NaCl (mp-22862) <1 0 0> <0 0 1> 0.259 258.5
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.268 256.4
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.270 316.5
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.287 179.4
SiC (mp-7631) <1 1 1> <0 0 1> 0.317 163.5
Ni (mp-23) <1 1 1> <0 0 1> 0.326 21.1
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.328 189.9
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.344 184.6
TePb (mp-19717) <1 0 0> <1 0 0> 0.390 222.1
TeO2 (mp-2125) <1 0 0> <0 0 1> 0.420 211.0
Si (mp-149) <1 0 0> <1 0 0> 0.443 185.1
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.461 100.2
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.465 185.1
TePb (mp-19717) <1 1 1> <0 0 1> 0.477 226.8
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.481 79.1
GaN (mp-804) <1 1 1> <0 0 1> 0.549 184.6
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.560 211.0
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.588 128.2
PbS (mp-21276) <1 1 1> <0 0 1> 0.608 63.3
C (mp-48) <1 1 1> <0 0 1> 0.628 100.2
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.655 279.6
WSe2 (mp-1821) <1 1 0> <1 1 0> 0.660 256.4
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.661 148.1
WSe2 (mp-1821) <1 1 1> <1 1 0> 0.662 256.4
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.667 110.8
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.670 148.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.696 36.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
786 182 25 0 0 0
182 786 25 0 0 0
25 25 50 0 0 0
0 0 0 -2 0 0
0 0 0 0 -2 0
0 0 0 0 0 302
Compliance Tensor Sij (10-12Pa-1)
1.4 -0.3 -0.5 0 0 -0.0
-0.3 1.4 -0.5 0 0 -0.0
-0.5 -0.5 20.7 0 0 0.0
0 0 0 -653.1 -0.0 0
0 0 0 -0.0 -653.1 0
-0.0 0.0 0.0 0 0 3.3
Shear Modulus GV
152 GPa
Bulk Modulus KV
232 GPa
Shear Modulus GR
-4 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
74 GPa
Bulk Modulus KVRH
140 GPa
Elastic Anisotropy
-194.73
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
B3C10N3 (mp-642462) 0.2875 0.584 3
BN (mp-629015) 0.2294 0.004 2
GaN (mp-1007824) 0.3046 0.355 2
BN (mp-685145) 0.2508 0.006 2
BN (mp-7991) 0.1503 0.000 2
BN (mp-604884) 0.2491 0.005 2
C (mp-568286) 0.1397 0.000 1
C (mp-990448) 0.0182 0.003 1
C (mp-48) 0.1199 0.001 1
C (mp-1040425) 0.0242 0.004 1
C (mp-1018088) 0.1342 1.299 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: C
Final Energy/Atom
-9.2219 eV
Corrected Energy
-36.8876 eV
-36.8876 eV = -36.8876 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)