File:LiCoO2-Li3PS4 interface reaction GC table MP.png

From Wiki
Jump to: navigation, search
Original file(1,322 × 1,264 pixels, file size: 524 KB, MIME type: image/png)

Table containing information for reaction between LiCoO2 and Li3PS4 in a open system to Li at Li chemical potential -3 eV vs. Li metal.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current19:08, 4 April 2018Thumbnail for version as of 19:08, 4 April 20181,322 × 1,264 (524 KB)Yxiao (talk | contribs)Table containing information for reaction between LiCoO2 and Li3PS4 in a open system to Li at Li chemical potential -3 eV vs. Li metal.